| Category: | PS+PE , Polystyrene + PE |
| Manufacturer: | NOVA Chemicals |
| Trademark: | ARCEL® |
| Fillers: | - |
| Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
| Delivery Terms | FOB, CIF, DAP, DAT, DDP |
| PDF: | E7Rf7r_ARCEL-640-3-00-pcf-.pdf |
| PRICE: | Order Products email sales@su-jiao.com |
| Message |
|---|
|
ARCEL® 640 (3.00 pcf) is a Polystyrene + PE (PS+PE) material. It is available in North America for foam processing. Typical application of ARCEL® 640 (3.00 pcf): Foam |
| General Information | |
|---|---|
| Features |
|
| Uses |
|
| Appearance |
|
| Forms |
|
| Processing Method |
|
| Physical | Nominal Value | Unit | |
|---|---|---|---|
| Density | 0.0481 | g/cm³ | |
| Particle Size - 98% | 0.700 to 1.40 | mm | |
| VOC Content | |||
| Pentane | 9.2 | % | |
| Plasticizer | 0.30 | % |
| Mechanical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Flexural Strength (5.0% Strain) | 0.456 | MPa | ASTM C203 |
| Compressive Strength | ASTM D1621 | ||
| 25% Strain | 0.274 | MPa | |
| 50% Strain | 0.369 | MPa | |
| 75% Strain | 0.693 | MPa |
| Elastomers | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Tensile Strength (Break) | 0.550 | MPa | ASTM D412 |
| Tensile Elongation (Break) | 10 | % | ASTM D412 |
| Flammability | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Burning Rate | 49 | mm/min | FMVSS 302 |
| Resin Grade | Manufacturer | Category | Trademark |
|---|---|---|---|
| Sarlink® TPE ML-1170B BLK X (PRELIMINARY DATA) | Teknor Apex Company | TPE | Sarlink® TPE |
| APEX® 2560-H | Teknor Apex Company | PVC, Flexible | APEX® |
| HAIPLEN EP50 X2 | Taro Plast S.p.A. | PP Copolymer | HAIPLEN |
| LNP™ THERMOCOMP™ UX06032 compound | SABIC Innovative Plastics Europe | PPA | LNP™ THERMOCOMP™ |
| Aquathene® CM92949B | LyondellBasell Industries | Polyolefin, Unspecified | Aquathene® |