Polyamide 66, %30 glass fiber reinforced, V0 flammability |
General Information | |
---|---|
Filler / Reinforcement |
|
Recycled Content |
|
Physical | Nominal Value | Unit | Test Method |
---|---|---|---|
Density | 1.32 to 1.36 | g/cm³ | ISO 1183 |
Molding Shrinkage | 0.25 to 0.35 | % |
Hardness | Nominal Value | Unit | Test Method |
---|---|---|---|
Shore Hardness (Shore D) | 80 to 85 | ISO 868 |
Mechanical | Nominal Value | Unit | Test Method |
---|---|---|---|
Tensile Modulus | 7500 to 10000 | MPa | ISO 527-2 |
Tensile Stress (Yield) | 120 to 150 | MPa | ISO 527-2 |
Tensile Strain (Break) | > 3.0 | % | ISO 527-2 |
Impact | Nominal Value | Unit | Test Method |
---|---|---|---|
Notched Izod Impact Strength | > 10 | kJ/m² | ISO 180/1A |
Thermal | Nominal Value | Unit | Test Method |
---|---|---|---|
Heat Deflection Temperature (1.8 MPa, Unannealed) | 250 | °C | ISO 75-2/A |
Vicat Softening Temperature | 255 | °C | ISO 306/B |
Melting Temperature (DSC) | 265 | °C | ISO 3146 |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
Tenopom® POM B3 V20 NTLA010 PR326 | Petropol Industry and Trade of Polymers LTDA | Acetal (POM) Copolymer | Tenopom® POM |
Karina GREEN PVC COMPOUND 450-DA-40/319-ATB | Karina Ind. e Com. de Plásticos Ltda | PVC, Unspecified | Karina |
Karina MBU BLUE(OP) -E 06/ 30-FC-HSF | Karina Ind. e Com. de Plásticos Ltda | PVC, Unspecified | Karina |
OnFlex™ S FR 70A-3S1890 | PolyOne Corporation | TPE | OnFlex™ |
3M™ Dyneon™ Fluoroelastomer FPO 3730 | 3M Advanced Materials Division | Fluorelastomer | 3M™ Dyneon™ Fluoroelastomer |