Category: | TPU-Polyether , Thermoplastic Polyurethane Elastomer (Polyether) |
Manufacturer: | Lubrizol Advanced Materials, Inc. |
Trademark: | Estane® |
Fillers: | - |
Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
Delivery Terms | FOB, CIF, DAP, DAT, DDP |
PDF: | DKCSgA_Estane-58123-TPU.pdf ![]() |
PRICE: | Order Products email sales@su-jiao.com |
Message |
---|
Type: Polyether Thermoplastic Polyurethane (TPU) Special Feature: Moisture Vapor Transmission, with Excellent Low Temperature and Elasticity. Low Moisture Absorption Processes: Extrusion: Blown, Flat Die Cast Film, Injection and Cable Jacketing |
General Information | |
---|---|
Features |
|
Uses |
|
Agency Ratings |
|
RoHS Compliance |
|
Appearance |
|
Forms |
|
Processing Method |
|
Physical | Nominal Value | Unit | Test Method |
---|---|---|---|
Specific Gravity | 1.06 | g/cm³ | ASTM D792 |
Hardness | Nominal Value | Unit | Test Method |
---|---|---|---|
Durometer Hardness (Shore A) | 70 | ASTM D2240 |
Mechanical | Nominal Value | Unit | Test Method |
---|---|---|---|
Taber Abrasion Resistance (1000 Cycles, 1000 g, H-18 Wheel) | 17.0 | mg | ASTM D3389 |
Films | Nominal Value | Unit | Test Method |
---|---|---|---|
Water Vapor Transmission | 420 | g/m²/24 hr | ASTM E96 |
Water Vapor Transmission - Mocon 1(38°C) | 3200 | g/m²/24 hr | ASTM D6701 |
Thermal | Nominal Value | Unit | Test Method |
---|---|---|---|
Kofler Melting Temperature | 150 | °C | Internal method |
Elastomers | Nominal Value | Unit | Test Method |
---|---|---|---|
Tensile Set (200% Strain) | 6 | % | ASTM D412 |
Tensile Stress | ASTM D412 | ||
100% strain | 3.40 | MPa | ASTM D412 |
300% strain | 5.50 | MPa | ASTM D412 |
Tensile Strength (Break) | 36.5 | MPa | ASTM D412 |
Tensile Elongation (Break) | 730 | % | ASTM D412 |
Tear Strength | |||
-- 2 | 66.7 | kN/m | ASTM D624 |
Cracking | 20 | kN/m | ASTM D470 |
Thermal | Nominal Value | Unit | Test Method |
---|---|---|---|
Glass Transition Temperature | -70.0 | °C | ASTM D3418 |
Melting Temperature | 135 | °C | DSC |
Extrusion | Nominal Value | Unit | |
---|---|---|---|
Drying Temperature | 180 | °C | |
Drying Time | 2.0 - 4.0 | hr | |
Suggested Max Moisture | 0.020 | % | |
Cylinder Zone 1 Temp. | 171 | °C | |
Cylinder Zone 2 Temp. | 177 | °C | |
Cylinder Zone 3 Temp. | 182 | °C | |
Cylinder Zone 4 Temp. | 188 | °C | |
Adapter Temperature | 193 | °C | |
Melt Temperature | 191 | °C | |
Die Temperature | 193 | °C |
Extrusion instructions |
---|
Dew Point: -40°CScreen Pack: 20/40/80 mesh |
Note Message | |
---|---|
1 . | 90% RH |
2 . | C mould |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
Starflam PFB139E | Eurostar Engineering Plastics | Nylon 6 | Starflam |
Novalloy-A A2606 | PlastxWorld Inc. | ABS+Nylon | Novalloy-A |
CENUSIL® R 150 | Wacker Chemie AG | Silicone | CENUSIL® |
ELASTOSIL® LR 3842/40 A/B | Wacker Chemie AG | Silicone | ELASTOSIL® LR |
Hanwha Total PE 431G | HANWHA TOTAL PETROCHEMICALS Co., Ltd. | LDPE | Hanwha Total PE |