| Category: | HPPA , HIGH PERFORMANCE POLYAMIDE RESIN |
| Manufacturer: | DuPont Performance Polymers |
| Trademark: | Zytel® HTN |
| Fillers: | - |
| Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
| Delivery Terms | FOB, CIF, DAP, DAT, DDP |
| PDF: | CtgL9N_ZytelHTN53C40HSLBK544.pdf |
| PRICE: | Order Products email sales@su-jiao.com |
| Message |
|---|
| 40% Carbon Fiber Reinforced High Performance Polyamide |
| General Information | |
|---|---|
| Filler / Reinforcement |
|
| Additive |
|
| Features |
|
| RoHS Compliance |
|
| Forms |
|
| Processing Method |
|
| Multi-Point Data |
|
| Part Marking Code (ISO 11469) |
|
| Resin ID (ISO 1043) |
|
| Physical | Dry | Conditioned | Unit | Test Method |
|---|---|---|---|---|
| Density | 1.31 | -- | g/cm³ | ISO 1183 |
| Mechanical | Dry | Conditioned | Unit | Test Method |
|---|---|---|---|---|
| Tensile Modulus | 28000 | 25000 | MPa | ISO 527-2 |
| Tensile Stress (Break) | 240 | 200 | MPa | ISO 527-2 |
| Tensile Strain (Break) | 1.7 | 1.9 | % | ISO 527-2 |
| Flexural Modulus | 26000 | -- | MPa | ISO 178 |
| Flexural Stress | 350 | -- | MPa | ISO 178 |
| Impact | Dry | Conditioned | Unit | Test Method |
|---|---|---|---|---|
| Charpy Notched Impact Strength (23°C) | 8.0 | -- | kJ/m² | ISO 179/1eA |
| Charpy Unnotched Impact Strength (23°C) | 60 | -- | kJ/m² | ISO 179/1eU |
| Thermal | Dry | Conditioned | Unit | Test Method |
|---|---|---|---|---|
| Heat Deflection Temperature (1.8 MPa, Unannealed) | 227 | -- | °C | ISO 75-2/A |
| Melting Temperature 1 | 260 | -- | °C | ISO 11357-3 |
| Electrical | Dry | Conditioned | Unit | Test Method |
|---|---|---|---|---|
| Volume Resistivity | 1.0E+3 | -- | ohms·cm | ASTM D4496 |
| Flammability | Dry | Conditioned | Unit | Test Method |
|---|---|---|---|---|
| Burning Rate 2(1.00 mm) | < 100 | -- | mm/min | ISO 3795 |
| FMVSS Flammability | B | -- | FMVSS 302 |
| Injection | Dry | Unit | |
|---|---|---|---|
| Melt Temperature, Optimum | 290 | °C | |
| Drying Recommended | yes | ||
| Drying Temperature | 100 | °C | |
| Drying Time - Desiccant Dryer | 6.0 - 8.0 | hr | |
| Suggested Max Moisture | 0.10 | % | |
| Processing (Melt) Temp | 280 - 300 | °C | |
| Mold Temperature | 90 - 110 | °C |
| Note Message | |
|---|---|
| 1 . | 10°C/min |
| 2 . | FMVSS 302 |
| Resin Grade | Manufacturer | Category | Trademark |
|---|---|---|---|
| SEETEC EVA VA810 | Lotte Chemical Corporation | EVA | SEETEC EVA |
| CALIBRE™ 320 UV | Trinseo | PC | CALIBRE™ |
| Arnitel® PB420-B | DSM Engineering Plastics | TPC-ET | Arnitel® |
| Delrin® 100PE BK602 | DuPont Performance Polymers | Acetal (POM) Homopolymer | Delrin® |
| Hapflex™ 595-3 | Hapco Inc. | TP, Unspecified | Hapflex™ |