| Category: | TPU-Polyester , Thermoplastic Polyurethane Elastomer (Polyester) |
| Manufacturer: | Shanghai Utomer Material Science Co., Ltd. |
| Trademark: | Utomer |
| Fillers: | - |
| Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
| Delivery Terms | FOB, CIF, DAP, DAT, DDP |
| PDF: | ClNhpf_Utomer-T795A.pdf |
| PRICE: | Order Products email sales@su-jiao.com |
| Message |
|---|
| Utomer T795A is a Thermoplastic Polyurethane Elastomer (Polyester) (TPU-Polyester) product. It is available in Asia Pacific. |
| General Information |
|---|
| Physical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Specific Gravity | 1.20 | g/cm³ | ASTM D792 |
| Melt Mass-Flow Rate (MFR) | 20 to 40 | g/10 min | ASTM D1238 |
| Hardness | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Durometer Hardness (Shore A) | 92 to 98 | ASTM D2240 |
| Elastomers | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Tensile Stress | ASTM D412 | ||
| 100% Strain | > 6.00 | MPa | |
| 300% Strain | > 18.0 | MPa | |
| Tensile Strength | > 35.0 | MPa | ASTM D412 |
| Tensile Elongation (Break) | > 500 | % | ASTM D412 |
| Tear Strength | > 0.110 | kN/m | ASTM D624 |
| Thermal | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Glass Transition Temperature | -10.0 | °C | ASTM D3418 |
| Resin Grade | Manufacturer | Category | Trademark |
|---|---|---|---|
| VENYL UG207 - 8071 | AD majoris | Nylon 66 | VENYL |
| Ekalon® 20 E I S | Sattler KunststoffWerk GmbH | PC | Ekalon® |
| HONES® PA66 G30 | Guangdong Shunde Hones Polymer Material Co., Ltd. | Nylon 66 | HONES® |
| Hostalen CRP 100 RT black | LyondellBasell Industries | HDPE | Hostalen |
| KumhoSunny ABS 770SR | Shanghai KumhoSunny Plastics Co., Ltd. | ABS | KumhoSunny ABS |