| Category: | Nylon 12 , Polyamide 12 |
| Manufacturer: | Arkema |
| Trademark: | Rilsan® |
| Fillers: | - |
| Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
| Delivery Terms | FOB, CIF, DAP, DAT, DDP |
| PDF: | CMIZ6w_Rilsan-ASR-30.pdf |
| PRICE: | Order Products email sales@su-jiao.com |
| Message |
|---|
|
Rilsan® ASR 30 is a Polyamide 12 (Nylon 12) product filled with filler. It can be processed by injection molding and is available in Africa & Middle East, Asia Pacific, Europe, Latin America, or North America. Characteristics include:
|
| General Information | |
|---|---|
| Filler / Reinforcement |
|
| Additive |
|
| Features |
|
| Forms |
|
| Processing Method |
|
| Physical | Dry | Conditioned | Unit | Test Method |
|---|---|---|---|---|
| Density | 1150 | 1150 | kg/m³ | ISO 1183 1 |
| Melt volume-flow rate (235°C/2.16 kg) | 3.00 | -- | cm³/10min | ISO 1133 2 |
| Mechanical | Dry | Conditioned | Unit | Test Method |
|---|---|---|---|---|
| Tensile modulus | 15000 | 14000 | MPa | ISO 527-2 3 |
| Tensile Stress (Break) | 161 | 154 | MPa | ISO 527-2 4 |
| Tensile Strain (Break) | 3.0 | 3.0 | % | ISO 527-2 5 |
| Impact | Dry | Conditioned | Unit | Test Method |
|---|---|---|---|---|
| Charpy notched impact strength | ISO 179/1eA 6 | |||
| -30°C | 9.00 | 9.00 | kJ/m² | |
| 23°C | 15.0 | 16.0 | kJ/m² | |
| Charpy impact strength | ISO 179/1eU 7 | |||
| -30°C | 59.0 | 59.0 | kJ/m² | |
| 23°C | 61.0 | 59.0 | kJ/m² |
| Thermal | Dry | Conditioned | Unit | Test Method |
|---|---|---|---|---|
| Deflection Temperature Under Load | ISO 75-2 8 | |||
| 0.45 MPa | 175 | -- | °C | |
| 1.8 MPa | 162 | -- | °C | |
| Vicat Softening Temperature (50°C/h, B (50N)) | 170 | -- | °C | ISO 306 9 |
| Melting Temperature 10 | 178 | -- | °C | ISO 11357-3 11 |
| CLTE - Flow | 4.0E-5 | -- | cm/cm/°C | ISO 11359-2 12 |
| Electrical | Dry | Conditioned | Unit | Test Method |
|---|---|---|---|---|
| Volume resistivity | -- | 4.0 | ohms·m | IEC 60093 13 |
| Comparative tracking index | -- | 100 | IEC 60112 14 |
| Flammability | Dry | Conditioned | Unit | Test Method |
|---|---|---|---|---|
| Burning Behav. at 1.6mm nom. thickn. (1.60 mm) | HB | -- | ISO 1210 15 | |
| Burning Behav. at thickness h (3.20 mm) | HB | -- | ISO 1210 16 |
| Note Message | |
|---|---|
| 1 . | Tested in accordance with ISO 10350. 23°C/50%r.h. unless otherwise noted. |
| 2 . | Tested in accordance with ISO 10350. 23°C/50%r.h. unless otherwise noted. |
| 3 . | Tested in accordance with ISO 10350. 23°C/50%r.h. unless otherwise noted. |
| 4 . | Tested in accordance with ISO 10350. 23°C/50%r.h. unless otherwise noted. |
| 5 . | Tested in accordance with ISO 10350. 23°C/50%r.h. unless otherwise noted. |
| 6 . | Tested in accordance with ISO 10350. 23°C/50%r.h. unless otherwise noted. |
| 7 . | Tested in accordance with ISO 10350. 23°C/50%r.h. unless otherwise noted. |
| 8 . | Tested in accordance with ISO 10350. 23°C/50%r.h. unless otherwise noted. |
| 9 . | Tested in accordance with ISO 10350. 23°C/50%r.h. unless otherwise noted. |
| 10 . | 10 °C/min |
| 11 . | Tested in accordance with ISO 10350. 23°C/50%r.h. unless otherwise noted. |
| 12 . | Tested in accordance with ISO 10350. 23°C/50%r.h. unless otherwise noted. |
| 13 . | Tested in accordance with ISO 10350. 23°C/50%r.h. unless otherwise noted. |
| 14 . | Tested in accordance with ISO 10350. 23°C/50%r.h. unless otherwise noted. |
| 15 . | Tested in accordance with ISO 10350. 23°C/50%r.h. unless otherwise noted. |
| 16 . | Tested in accordance with ISO 10350. 23°C/50%r.h. unless otherwise noted. |
| Resin Grade | Manufacturer | Category | Trademark |
|---|---|---|---|
| Monprene® OM-10165 | Teknor Apex Company | TPE | Monprene® |
| KRYSTALFLEX™ PE409 | Huntsman Corporation | PUR-Eth,aliphat | KRYSTALFLEX™ |
| Karina OCHER PVC COMPOUND 810-37/3-CRB | Karina Ind. e Com. de Plásticos Ltda | PVC, Unspecified | Karina |
| LOFEX® A41AA | Lotte Chemical Corporation | PET | LOFEX® |
| Plenco 07507 (Transfer) | Plastics Engineering Co. | Phenolic | Plenco |