| Message |
|---|
| Super High Impact/Good Processability |
| General Information | |
|---|---|
| Features |
|
| Forms |
|
| Physical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Specific Gravity | 1.03 | g/cm³ | ASTM D792 |
| Melt Mass-Flow Rate (MFR) (220°C/10.0 kg) | 3.0 - 7.0 | g/10 min | ASTM D1238 |
| Hardness | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Rockwell Hardness (R-Scale, 23°C) | 100 | ASTM D785 |
| Mechanical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Tensile Strength 1 | ASTM D638 | ||
| Yield, 23°C, 3.18mm | 34.3 | MPa | ASTM D638 |
| Fracture, 23°C, 3.18mm | 29.4 | MPa | ASTM D638 |
| Flexural Strength 2(Yield, 23°C) | 58.8 | MPa | ASTM D790 |
| Impact | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Notched Izod Impact (23°C) | 370 - 410 | J/m | ASTM D256A |
| Thermal | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Deflection Temperature Under Load (1.8 MPa, Unannealed) | 85.0 | °C | ASTM D648 |
| Flammability | Nominal Value | Test Method | |
|---|---|---|---|
| Flame Rating (1.6 mm) | HB | UL 94 |
| Note Message | |
|---|---|
| 1 . | 5.0 mm/min |
| 2 . | 2.8 mm/min |
| Resin Grade | Manufacturer | Category | Trademark |
|---|---|---|---|
| Tarflen® DE | Grupa Azoty S.A. | PTFE | Tarflen® |
| Mylar® A (1000 guage) | DuPont Teijin Films U.S. | PET | Mylar® |
| Aegis® H95XC | Honeywell | Nylon 6 | Aegis® |
| Diamond ASA S170 | Network Polymers, Inc. | ASA | Diamond ASA |
| Vipel® F701-S-SPT-23 | AOC, L.L.C. | Polyester Alloy | Vipel® |