Category: | Nylon 66 , Polyamide 66 |
Manufacturer: | Solvay Engineering Plastics |
Trademark: | TECHNYL® |
Fillers: | - |
Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
Delivery Terms | FOB, CIF, DAP, DAT, DDP |
PDF: | C5r0eX_TECHNYLA238V13BLACK21N.pdf ![]() |
PRICE: | Order Products email sales@su-jiao.com |
Message |
---|
TECHNYL® A 238 V13 Black 21N is a polyamide 6.6, reinforced with 13% of glass fiber, heat stabilized, impact modified, for injection moulding. This grade offers excellent combination between rigidity and impact resistance at ambient temperature. |
General Information | |
---|---|
Filler / Reinforcement |
|
Additive |
|
Features |
|
Uses |
|
Agency Ratings |
|
RoHS Compliance |
|
Appearance |
|
Forms |
|
Processing Method |
|
Resin ID (ISO 1043) |
|
Mechanical | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Tensile Modulus (23°C) | 5500 | 3650 | MPa | ISO 527-2/1A |
Tensile Stress (Yield, 23°C) | 100 | 60.0 | MPa | ISO 527-2/1A |
Tensile Strain (Yield, 23°C) | 4.0 | 8.0 | % | ISO 527-2 |
Impact | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Charpy Notched Impact Strength (23°C) | 6.0 | 8.0 | kJ/m² | ISO 179/1eA |
Charpy Unnotched Impact Strength (23°C) | 65 | 60 | kJ/m² | ISO 179/1eU |
Notched Izod Impact (23°C) | 8.0 | 10 | kJ/m² | ISO 180 |
Thermal | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Heat Deflection Temperature (1.8 MPa, Unannealed) | 228 | -- | °C | ISO 75-2/Af |
Melting Temperature | 263 | -- | °C | ISO 11357-3 |
Flammability | Dry | Conditioned | Test Method | |
---|---|---|---|---|
Flame Rating (1.6 mm) | HB | -- | UL 94 |
Injection | Dry | Unit | |
---|---|---|---|
Drying Temperature | 80 | °C | |
Suggested Max Moisture | 0.20 | % | |
Rear Temperature | 270 - 280 | °C | |
Middle Temperature | 275 - 285 | °C | |
Front Temperature | 280 - 290 | °C | |
Mold Temperature | 70 - 100 | °C |
Injection instructions |
---|
The material is supplied in airtight bags, ready for use. In case that the virgin material has absorbed moisture, it must be dried with a dehumidified air drying equipment, dew point mini -20°C. Recommended time 2-4hInjection Advice: For reinforced polyamide, Solvay recommends the use of steel with a high content of Carbon and purified for polishing to avoid or limit the abrasion. For example: X38CrMoV5-1 (EN Norm) - 1.2367 /1.2343 (DIN Norm) or X160CrMoV12 (EN Norm) - 1.2601 /1.2379 (DIN Norm). For Mould Temperature, in the case of parts where the surface roughness is required we can recommend a temperature of 90°C to 120°C with an optimum at 105°C. The processing parameters like processing temperatures are a recommendation and can be adjusted in function of injection machine size, part geometry / design |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
TABOREN EC 59 C 50 | SILON s.ro | LLDPE | TABOREN |
Next Nylon 66 Prime Series PXH-01NC | Next Polymers Ltd. | Nylon 66 | Next Nylon 66 Prime Series |
ASI POLYPROPYLENE 3515 | A. Schulman Inc. | PP Copolymer | ASI POLYPROPYLENE |
OP - PBT 15GF-FR | Oxford Polymers | PBT | OP - PBT |
CYCOLAC™ INP338 resin | SABIC Innovative Plastics | ABS | CYCOLAC™ |