HHP-849 is a certified prime, natural color base hexene-copolymer grade, designed for EXTRUSION of PIPE. HHP-849 meets PE-3408 non-pressure and pressure pipe service requirements from 1 to 64 inch sized diameters and features good long-term hoop strength performance for applications including municipal potable water pipe, fuel gas pipe, re-lining pipe, industrial and mining pipe, storm and sanitary pipe. HHP-849 processing temperature is 365° to 390°F (185° to 199°C). HHP-849 meets all requirements of ASTM-D4976 - PE 235 & NSF Standard 14/61. |
General Information | |
---|---|
Features |
|
Uses |
|
Agency Ratings |
|
Appearance |
|
Forms |
|
Processing Method |
|
Physical | Nominal Value | Unit | Test Method |
---|---|---|---|
Density | 0.949 | g/cm³ | ASTM D1505 |
Melt Mass-Flow Rate (MFR) | ASTM D1238 | ||
190°C/2.16 kg | 0.080 | g/10 min | ASTM D1238 |
190°C/21.6 kg | 8.0 | g/10 min | ASTM D1238 |
Environmental Stress-Cracking Resistance 1(100°C, 1.75mm, 100% Igepal, molding, F50) | > 5000 | hr | ASTM D1693C |
Mechanical | Nominal Value | Unit | Test Method |
---|---|---|---|
Tensile Strength 2(Yield, Compression Molded) | 23.0 | MPa | ASTM D638 |
Tensile Elongation 3(Break, Compression Molded) | 850 | % | ASTM D638 |
Flexural Modulus - 2% Secant 4(Compression Molded) | 850 | MPa | ASTM D790 |
Slow crack propagation PENT | > 100 | hr | ASTM F1473 |
Additional Information | Nominal Value | Test Method | |
---|---|---|---|
Unit classification | PE 345464A | ASTM D3350 |
Impact | Nominal Value | Unit | Test Method |
---|---|---|---|
Notched Izod Impact (23°C, Compression Molded) | 37 | J/m | ASTM D256 |
Thermal | Nominal Value | Unit | Test Method |
---|---|---|---|
Brittleness Temperature | < -100 | °C | ASTM D746 |
Vicat Softening Temperature | 124 | °C | ASTM D1525 |
Additional Information | Nominal Value | Test Method | |
---|---|---|---|
Test specimens from compression molded plaque according to ASTM D 1928 Procedure C. |
Extrusion | Nominal Value | Unit | |
---|---|---|---|
Melt Temperature | 185 - 199 | °C |
Note Message | |
---|---|
1 . | Notched Bent Strip |
2 . | 50 mm/min |
3 . | 50 mm/min |
4 . | 1.3 mm/min |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
NEOFLON™ EC-6516 | DAIKIN AMERICA, INC. | ETFE | NEOFLON™ |
Abstron PT45M | Bhansali Engineering Polymers Limited | ABS | Abstron |
INSTRUC PPGF10 | Infinity LTL Engineered Compounds | PP, Unspecified | INSTRUC |
EMERGE™ PC 8130-15 | Trinseo | PC | EMERGE™ |
LGG 105 | LG Polymers India Pvt. Ltd. | PS (GPPS) | LGG |