Elexar®EL-1446A is a thermoplastic elastomer (TPE) material,. This product is available in North America, Africa and the Middle East, Latin America, Europe or Asia Pacific. The processing method is extrusion or injection molding. Elexar®The main characteristics of the EL-1446A are: flame retardant/rated flame. Typical application areas include:
|
General Information | |
---|---|
Uses |
|
Appearance |
|
Forms |
|
Processing Method |
|
Physical | Nominal Value | Unit | Test Method |
---|---|---|---|
Specific Gravity | 1.25 | g/cm³ | ASTM D792 |
Melt Mass-Flow Rate (MFR) (200°C/5.0 kg) | 18 | g/10 min | ASTM D1238 |
Hardness | Nominal Value | Unit | Test Method |
---|---|---|---|
Durometer Hardness | ASTM D2240 | ||
Shaw A | 93 | ASTM D2240 | |
Shaw D, 15 seconds | 36 | ASTM D2240 |
Elastomers | Nominal Value | Unit | Test Method |
---|---|---|---|
Tensile Strength (Break) | 12.4 | MPa | ASTM D412 |
Tensile Elongation (Break) | 530 | % | ASTM D412 |
Aging | Nominal Value | Unit | Test Method |
---|---|---|---|
Change in Tensile Strength (158°C, 168 hr) | 3.0 | % | ASTM D471 |
Change in Ultimate Elongation (158°C, 168 hr) | -13 | % | ASTM D471 |
Thermal | Nominal Value | Unit | Test Method |
---|---|---|---|
Brittleness Temperature | < -50.0 | °C | ASTM D746 |
Flammability | Nominal Value | Unit | Test Method |
---|---|---|---|
Flame Rating (1.52 mm) | V-0 | UL 94 | |
Oxygen Index | 27 | % | ASTM D2863 |
Injection | Nominal Value | Unit | |
---|---|---|---|
Rear Temperature | 199 - 216 | °C | |
Middle Temperature | 213 - 221 | °C | |
Front Temperature | 221 - 227 | °C | |
Nozzle Temperature | 221 - 229 | °C | |
Processing (Melt) Temp | 221 - 229 | °C | |
Mold Temperature | 25.0 - 65.6 | °C | |
Injection Pressure | 1.38 - 6.89 | MPa | |
Injection Rate | Moderate-Fast | ||
Back Pressure | 0.172 - 0.345 | MPa | |
Screw Speed | 50 - 100 | rpm | |
Cushion | 3.81 - 25.4 | mm |
Injection instructions |
---|
无需干燥。但如果湿度过大,则将粒料在150°F (65°C)的温度下干燥2-4小时。 |
Extrusion | Nominal Value | Unit | |
---|---|---|---|
Cylinder Zone 1 Temp. | 193 - 210 | °C | |
Cylinder Zone 2 Temp. | 199 - 216 | °C | |
Cylinder Zone 3 Temp. | 213 - 221 | °C | |
Cylinder Zone 5 Temp. | 221 - 227 | °C | |
Die Temperature | 221 - 229 | °C |
Extrusion instructions |
---|
螺杆转速30 - 100 rpm |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
MARPOL® RCopo 1.8.CL | Marco Polo International, Inc. | PP Random Copolymer | MARPOL® RCopo |
RTP 200 GB 23 | RTP Company | Nylon 66 | RTP |
RTP 800 AR 15 TFE 15 | RTP Company | Acetal (POM) Copolymer | RTP |
Arnite® XG 260 S (T-X07086) | DSM Engineering Plastics | PBT | Arnite® |
Dyna-Purge® C | Dyna-Purge, division of Shuman Plastics | Proprietary | Dyna-Purge® |