| Category: | Nylon 6 , Polyamide 6 |
| Manufacturer: | Solvay Engineering Plastics |
| Trademark: | TECHNYL® C |
| Fillers: | - |
| Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
| Delivery Terms | FOB, CIF, DAP, DAT, DDP |
| PDF: | BKKmt3_TECHNYL-C-218-V50-BLACK-51.pdf |
| PRICE: | Order Products email sales@su-jiao.com |
| Message |
|---|
| TECHNYL C 218 V50 is a polyamide 6 reinforced with 50% of glass fiber with excellent thermal stability |
| General Information | |
|---|---|
| Filler / Reinforcement |
|
| Features |
|
| Appearance |
|
| Processing Method |
|
| Physical | Dry | Conditioned | Unit | Test Method |
|---|---|---|---|---|
| Specific Gravity | 1.56 | -- | g/cm³ | ASTM D792 |
| Water Absorption (Equilibrium, 23°C, 50% RH) | 0.75 | -- | % | ISO 62 |
| Mechanical | Dry | Conditioned | Unit | Test Method |
|---|---|---|---|---|
| Tensile Modulus | 14600 | 8600 | MPa | ISO 527-2 |
| Tensile Stress | 225 | 150 | MPa | ISO 527-2 |
| Tensile Strain (Break) | 2.0 | 3.0 | % | ISO 527-2 |
| Impact | Dry | Conditioned | Unit | Test Method |
|---|---|---|---|---|
| Charpy Notched Impact Strength | 19 | 34 | kJ/m² | ISO 179 |
| Charpy Unnotched Impact Strength | 110 | 120 | kJ/m² | ISO 179 |
| Notched Izod Impact Strength | 17 | 29 | kJ/m² | ISO 180 |
| Thermal | Dry | Conditioned | Unit | Test Method |
|---|---|---|---|---|
| Heat Deflection Temperature (1.8 MPa, Unannealed) | 215 | -- | °C | ISO 75-2/A |
| Peak Melting Temperature | 222 | -- | °C | ASTM D3418 |
| Electrical | Dry | Conditioned | Unit | Test Method |
|---|---|---|---|---|
| Volume Resistivity | 1.0E+15 | 1.0E+11 | ohms·cm | IEC 60093 |
| Electric Strength | -- | 22 | kV/mm | IEC 60243-1 |
| Relative Permittivity (1 MHz) | 3.80 | 4.50 | IEC 60250 | |
| Dissipation Factor (1 MHz) | 0.020 | 9.0E-3 | IEC 60250 | |
| Comparative Tracking Index | 550 | 475 | V | IEC 60112 |
| Flammability | Dry | Conditioned | Unit | Test Method |
|---|---|---|---|---|
| Flame Rating (0.400 mm) | HB | -- | UL 94 | |
| Glow Wire Flammability Index (1.60 mm) | 650 | -- | °C | IEC 60695-2-12 |
| Oxygen Index | 23 | -- | % | ISO 4589-2 |
| Injection | Dry | Unit | |
|---|---|---|---|
| Rear Temperature | 225 to 230 | °C | |
| Middle Temperature | 230 to 240 | °C | |
| Front Temperature | 240 to 250 | °C | |
| Nozzle Temperature | 230 to 240 | °C | |
| Mold Temperature | 80.0 to 100 | °C |
| Resin Grade | Manufacturer | Category | Trademark |
|---|---|---|---|
| Borlink™ LE4244EHV | Borealis AG | PE, Unspecified | Borlink™ |
| Chemraz 656 | Greene, Tweed & Co. | Perfluoroelastomer | Chemraz |
| Grilon® TSM-40/4 | EMS-GRIVORY | Nylon 66/6 | Grilon® |
| Epoxies, Ect. 10-3002 | Epoxies, Etc. | Epoxy | Epoxies, Ect. |
| Karina MBU GRAY E 18/601-IE | Karina Ind. e Com. de Plásticos Ltda | PVC, Unspecified | Karina |