Category: | TPO (POE) , Thermoplastic Polyolefin Elastomer |
Manufacturer: | RTP Company |
Trademark: | RTP |
Fillers: | - |
Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
Delivery Terms | FOB, CIF, DAP, DAT, DDP |
PDF: | BIsEQ5_RTP-EMI-2862-75A.pdf ![]() |
PRICE: | Order Products email sales@su-jiao.com |
Message |
---|
Warning: The status of this material is 'Commercial: Limited Issue' The data for this material has not been recently verified. Please contact RTP Company for current information prior to specifying this grade. Stainless Steel Fiber - Electrically Conductive - EMI/RFI/ESD Protection |
General Information | |
---|---|
Filler / Reinforcement |
|
Features |
|
RoHS Compliance |
|
Processing Method |
|
Physical | Nominal Value | Unit | Test Method |
---|---|---|---|
Specific Gravity | 1.08 | g/cm³ | ASTM D792 |
Molding Shrinkage - Flow (3.20 mm) | 1.0 - 1.5 | % | ASTM D955 |
Moisture Content | 0.030 | % |
Electrical | Nominal Value | Unit | Test Method |
---|---|---|---|
Static Decay | sec | FTMS 101C 4046.1 |
Additional Information | Nominal Value | Unit | |
---|---|---|---|
Primary Additive | 15 | % |
Hardness | Nominal Value | Unit | Test Method |
---|---|---|---|
Durometer Hardness (Shore A, 10 sec) | 75 | ASTM D2240 |
Mechanical | Nominal Value | Unit | Test Method |
---|---|---|---|
Tensile Strength | 2.07 | MPa | ASTM D638 |
Tensile Elongation (Yield) | > 150 | % | ASTM D638 |
Impact | Nominal Value | Unit | Test Method |
---|---|---|---|
Notched Izod Impact (3.20 mm) | No Break | ASTM D256 | |
Unnotched Izod Impact (3.20 mm) | No Break | ASTM D4812 |
Electrical | Nominal Value | Unit | Test Method |
---|---|---|---|
Surface Resistivity | |||
-- 1 | < 1.0E+4 | ohms | ASTM D257 |
-- | < 1.0E+3 | ohms | ESD STM11.11 |
Volume Resistivity | < 10 | ohms·cm | ASTM D257 |
Injection | Nominal Value | Unit | |
---|---|---|---|
Drying Temperature | 79.4 | °C | |
Drying Time | 2.0 | hr | |
Dew Point | -17.8 | °C | |
Processing (Melt) Temp | 182 - 210 | °C | |
Mold Temperature | 15.6 - 65.6 | °C | |
Injection Pressure | 82.7 - 124 | MPa |
Injection instructions |
---|
Use a reverse barrel profile. Remove hopper magnets. Allow 4 - 5 shots to properly disperse the conductive fibers. The surface finish should have a silver streaking appearance, not clumps.Remove hopper magnets. |
Note Message | |
---|---|
1 . | ESD STM11.11 |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
Salflex 340D | Salflex Polymers Ltd. | TPV | Salflex |
DJSilicone NE-671 | DONGJUE SILICONE (NANJING) CO., LTD | Silicone | DJSilicone |
Huafon HF-4385A | Huafon Group Co., Ltd. | TPU-Polyether | Huafon |
Infino FD-1122 | SAMSUNG SDI CO., LTD. | PC | Infino |
Formolene® 6730L | Formosa Plastics Corporation, U.S.A. | PP Copolymer | Formolene® |