| Category: | PP, Unspecified , Polypropylene |
| Manufacturer: | TechnoCompound GmbH |
| Trademark: | TechnoFiber |
| Fillers: | - |
| Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
| Delivery Terms | FOB, CIF, DAP, DAT, DDP |
| PDF: | BG6Wa4_TechnoFiberPPLGF401001H.pdf |
| PRICE: | Order Products email sales@su-jiao.com |
| Message |
|---|
|
TechnoFiber: Strong and light TechnoFiber products are long glass fiber remforced thermoplastics made by TechnoCompound GmbH. These raw materials are fashioned into so-called tailor-made compounds upon customer specifications. Nearly all semi-crystalline and amorphous thermoplastics can be used as thermoplastic matrlx. Our long glass flber products are predestmed for the manufacturing of components which are exposed to extreme mechanical stress - as well as to high temperatures. The long glass fiber reinforced pellets are available in lengths of 10 - 25 mm. Fiber and pellet are of the same length. The two-step pultrusion technology applied by TechnoCompound coats each glass flber fllament wlth a polymer matrrx and JOINS flber and matrrx. Typical Applications
|
| General Information | |
|---|---|
| Filler / Reinforcement |
|
| Additive |
|
| Features |
|
| Uses |
|
| Appearance |
|
| Forms |
|
| Physical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Density | 1.20 | g/cm³ | ISO 1183 |
| shrinkage- Flow 1 | 0.20 | % | ISO 294-4 |
| Mechanical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Tensile Modulus | 8900 | MPa | ISO 527-2/1 |
| Tensile Stress (Yield) | 120 | MPa | ISO 527-2/50 |
| Tensile Strain (Yield) | 2.3 | % | ISO 527-2/50 |
| Flexural Modulus 2 | 9100 | MPa | ISO 178 |
| Flexural Stress 3 | 140 | MPa | ISO 178 |
| Impact | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Charpy Notched Impact Strength | ISO 179/1eA | ||
| -30°C | 19 | kJ/m² | ISO 179/1eA |
| 23°C | 20 | kJ/m² | ISO 179/1eA |
| Charpy Unnotched Impact Strength | ISO 179/1eU | ||
| -30°C | 54 | kJ/m² | ISO 179/1eU |
| 23°C | 58 | kJ/m² | ISO 179/1eU |
| Thermal | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Heat Deflection Temperature | |||
| 0.45 MPa, not annealed | 160 | °C | ISO 75-2/B |
| 1.8 MPa, not annealed | 152 | °C | ISO 75-2/A |
| 8.0 MPa, not annealed | 128 | °C | ISO 75-2/C |
| Melting Temperature 4 | 165 | °C | ISO 11357-3 |
| Linear thermal expansion coefficient | ISO 11359-2 | ||
| Flow : 23 to 80°C | 1.5E-5 | cm/cm/°C | ISO 11359-2 |
| Lateral : 23 to 80°C | 3.4E-5 | cm/cm/°C | ISO 11359-2 |
| Note Message | |
|---|---|
| 1 . | 220°C / WZ 40°C, 600 bar |
| 2 . | 2.0 mm/min |
| 3 . | 5.0 mm/min |
| 4 . | 10°C/min |
| Resin Grade | Manufacturer | Category | Trademark |
|---|---|---|---|
| Ravago Compounds HMP-8660 | Ravago Manufacturing Americas, LLC | HDPE | Ravago Compounds |
| RapidCast™ RC-542 | Innovative Polymers, Inc. | TSU | RapidCast™ |
| Elastron® V V201.A40.N | Elastron USA, Inc. | TPV | Elastron® V |
| Ultradur® B 4040 G6 HR BK15029 | BASF Corporation | PBT+PET | Ultradur® |
| CYCOLAC™ FXS610SK resin | SABIC Innovative Plastics Europe | ABS | CYCOLAC™ |