| Category: | SBS , Styrene Butadiene Styrene Block Copolymer |
| Manufacturer: | SO.F.TER. SPA |
| Trademark: | Sofprene T® |
| Fillers: | - |
| Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
| Delivery Terms | FOB, CIF, DAP, DAT, DDP |
| PDF: | ANrZGs_Sofprene-T-540200A30.pdf |
| PRICE: | Order Products email sales@su-jiao.com |
| Message |
|---|
| Sofprene T® 540200A30 is a Styrene Butadiene Styrene Block Copolymer (SBS) material. It is available in Europe, Latin America, or North America for injection molding. Primary attribute of Sofprene T® 540200A30: REACH Compliant. |
| General Information | |
|---|---|
| Agency Ratings |
|
| Appearance |
|
| Processing Method |
|
| Physical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Specific Gravity | 1.04 | g/cm³ | ASTM D792 |
| Hardness | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Durometer Hardness (Shore A, 15 sec) | 30 | ASTM D2240 |
| Elastomers | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Tensile Set | 2 | % | ASTM D412 |
| Tensile Stress 1(100% Strain) | 0.800 | MPa | ASTM D412 |
| Tensile Strength 2 | 1.90 | MPa | ASTM D412 |
| Tensile Elongation 3(Break) | 720 | % | ASTM D412 |
| Tear Strength 4 | 21.0 | kN/m | ASTM D624 |
| Injection | Nominal Value | Unit | |
|---|---|---|---|
| Rear Temperature | 150 | °C | |
| Middle Temperature | 160 | °C | |
| Front Temperature | 170 | °C | |
| Nozzle Temperature | 175 | °C | |
| Mold Temperature | 20.0 to 40.0 | °C |
| Note Message | |
|---|---|
| 1 . | Die C |
| 2 . | Die C |
| 3 . | Die C |
| 4 . | Die C |
| Resin Grade | Manufacturer | Category | Trademark |
|---|---|---|---|
| RTP 202A HI | RTP Company | Nylon 6 | RTP |
| RTP EMI 332E FR | RTP Company | PC | RTP |
| Ultramid® 8202 L | BASF Corporation | Nylon 6 | Ultramid® |
| ASI POLYPROPYLENE 1255H-01 | A. Schulman Inc. | PP Homopolymer | ASI POLYPROPYLENE |
| Petrothene® NA336 | LyondellBasell Industries | LDPE | Petrothene® |