STERLENE™ CMV257A

Category: TPO (POE) , Thermoplastic Polyolefin Elastomer
Manufacturer: R&P (Pte.) Ltd.
Trademark: STERLENE™
Fillers: -
Ports: Qinzhou, Shekou, Shanghai, Ningbo
Delivery Terms FOB, CIF, DAP, DAT, DDP
PDF: ANkYUu_STERLENE-CMV257A.pdf
PRICE: ​Order Products​ email   sales@su-jiao.com
Wechat: WECHAT
Message
STERLENE™ CMV257A is a polyolefin injection molding compound designed for mold-in-color automotive interior trim applications. This product has medium melt flow, high stiffness and great scratch resistance.
General Information
Features
  • High Scratch Resistance
  • High Stiffness
  • Medium Flow
Uses
  • Automotive Applications
  • Automotive Interior Trim
Processing Method
  • Injection Molding
PhysicalNominal ValueUnitTest Method
Density 1.01g/cm³ISO 1183
Melt Mass-Flow Rate (MFR) 1(230°C/2.16 kg)19g/10 minISO 1133
MechanicalNominal ValueUnitTest Method
Tensile Modulus (23°C)2710MPaISO 527-2/50
Tensile Stress (Yield, 23°C)27.0MPaISO 527-2/50
Tensile Strain ISO 527-2/50
    Yield, 23°C 4.8%
    Break, 23°C 14%
Flexural Modulus 2(23°C)2400MPaISO 178
Flexural Stress 3(23°C)40.0MPaISO 178
ImpactNominal ValueUnitTest Method
Notched Izod Impact Strength (23°C, Complete Break)9.0kJ/m²ISO 180/A
ThermalNominal ValueUnitTest Method
Heat Deflection Temperature (1.8 MPa, Unannealed)59.0°CISO 75-2/Af
InjectionNominal ValueUnit
Drying Time 2.0hr
Processing (Melt) Temp 190 to 240°C
Mold Temperature 25.0 to 60.0°C
Note Message
1 .Procedure B
2 .2.0 mm/min
3 .2.0 mm/min
Resin Grade Manufacturer Category Trademark
AKROMID® B3 GF 15 RM-M natural (3697) AKRO-PLASTIC GmbH Nylon 6 AKROMID®
Andur M-22 (HQEE) Anderson Development Company PUR-Ester/MDI Andur
ARC ARC6604 ARC Resin Corporation Nylon 66 ARC
EMOPLEN® CP FR V0 EMAS Plastik San.Tic.AS. PP Copolymer EMOPLEN®
Extir® CM PD GALILEO IO M 5 AE Versalis S.p.A. PS (EPS) Extir®