Category: | PP, Unspecified , Polypropylene |
Manufacturer: | TechnoCompound GmbH |
Trademark: | TechnoFiber |
Fillers: | - |
Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
Delivery Terms | FOB, CIF, DAP, DAT, DDP |
PDF: | A7T7Y1_TechnoFiberPPLGF201001H.pdf ![]() |
PRICE: | Order Products email sales@su-jiao.com |
Message |
---|
TechnoFiber: Strong and light TechnoFiber products are long glass fiber remforced thermoplastics made by TechnoCompound GmbH. These raw materials are fashioned into so-called tailor-made compounds upon customer specifications. Nearly all semi-crystalline and amorphous thermoplastics can be used as thermoplastic matrlx. Our long glass flber products are predestmed for the manufacturing of components which are exposed to extreme mechanical stress - as well as to high temperatures. The long glass fiber reinforced pellets are available in lengths of 10 - 25 mm. Fiber and pellet are of the same length. The two-step pultrusion technology applied by TechnoCompound coats each glass flber fllament wlth a polymer matrrx and JOINS flber and matrrx. Typical Applications
|
General Information | |
---|---|
Filler / Reinforcement |
|
Additive |
|
Features |
|
Uses |
|
Appearance |
|
Forms |
|
Physical | Nominal Value | Unit | Test Method |
---|---|---|---|
Density | 1.03 | g/cm³ | ISO 1183 |
shrinkage- Flow 1 | 0.40 | % | ISO 294-4 |
Mechanical | Nominal Value | Unit | Test Method |
---|---|---|---|
Tensile Modulus | 4800 | MPa | ISO 527-2/1 |
Tensile Stress (Yield) | 95.0 | MPa | ISO 527-2/50 |
Tensile Strain (Yield) | 2.8 | % | ISO 527-2/50 |
Flexural Modulus 2 | 4900 | MPa | ISO 178 |
Flexural Stress 3 | 120 | MPa | ISO 178 |
Impact | Nominal Value | Unit | Test Method |
---|---|---|---|
Charpy Notched Impact Strength | ISO 179/1eA | ||
-30°C | 15 | kJ/m² | ISO 179/1eA |
23°C | 16 | kJ/m² | ISO 179/1eA |
Charpy Unnotched Impact Strength | ISO 179/1eU | ||
-30°C | 45 | kJ/m² | ISO 179/1eU |
23°C | 50 | kJ/m² | ISO 179/1eU |
Thermal | Nominal Value | Unit | Test Method |
---|---|---|---|
Heat Deflection Temperature (0.45 MPa, Unannealed) | 160 | °C | ISO 75-2/B |
Vicat Softening Temperature | 147 | °C | ISO 306/B120 |
Melting Temperature 4 | 165 | °C | ISO 11357-3 |
Linear thermal expansion coefficient | ISO 11359-2 | ||
Flow : 23 to 80°C | 1.8E-5 | cm/cm/°C | ISO 11359-2 |
Lateral : 23 to 80°C | 4.9E-5 | cm/cm/°C | ISO 11359-2 |
Note Message | |
---|---|
1 . | 220°C / WZ 40°C, 600 bar |
2 . | 2.0 mm/min |
3 . | 5.0 mm/min |
4 . | 10°C/min |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
TECHNO MUH LG5053 | Techno Polymer Co, Ltd. | ABS | TECHNO MUH |
TECHLEN GT217 | DAEHA Co., LTD | PP, Unspecified | TECHLEN |
VITAMIDE® TR26 | A. Schulman Europe | Nylon 66/6 | VITAMIDE® |
TOTAL Polypropylene PPH 3721WZ | TOTAL Refining & Chemicals | PP Homopolymer | TOTAL Polypropylene |
Aristech Quarite Select Plus® | Aristech Acrylics LLC | Acrylic, Unspecified | Aristech |