Category: | PP, Unspecified , Polypropylene |
Manufacturer: | Ferro Corporation |
Trademark: | GAPEX® |
Fillers: | - |
Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
Delivery Terms | FOB, CIF, DAP, DAT, DDP |
PDF: | A4CVxG_GAPEX-RPP10EU56BK.pdf ![]() |
PRICE: | Order Products email sales@su-jiao.com |
Message |
---|
GAPEX®RPP10EU56BK is a polypropylene material, and the filler is 10% glass fiber reinforced material. This product is available in North America, Africa and the Middle East, Latin America, Europe or Asia Pacific,. GAPEX®The main features of the RPP10EU56BK are:
|
General Information | |
---|---|
Filler / Reinforcement |
|
Additive |
|
Features |
|
Forms |
|
Physical | Nominal Value | Unit | Test Method |
---|---|---|---|
Specific Gravity | 0.968 | g/cm³ | ASTM D792 |
Melt Mass-Flow Rate (MFR) (230°C/2.16 kg) | 6.5 | g/10 min | ASTM D1238 |
Molding Shrinkage | ASTM D955 | ||
Flow | 0.70 | % | ASTM D955 |
Transverse flow | 1.0 | % | ASTM D955 |
Mechanical | Nominal Value | Unit | Test Method |
---|---|---|---|
Tensile Strength (23°C) | 42.7 | MPa | ASTM D638 |
Tensile Elongation (Break, 23°C) | 12 | % | ASTM D638 |
Flexural Modulus | ASTM D790 | ||
1% secant : 23°C | 2150 | MPa | ASTM D790 |
Tangent : 23°C | 2240 | MPa | ASTM D790 |
Flexural Strength (23°C) | 65.5 | MPa | ASTM D790 |
Impact | Nominal Value | Unit | Test Method |
---|---|---|---|
Notched Izod Impact (23°C) | 85 | J/m | ASTM D256 |
Unnotched Izod Impact (23°C) | 450 | J/m | ASTM D4812 |
Dart Drop Impact (23°C) | 0.904 | J | ASTM D5420 |
Thermal | Nominal Value | Unit | Test Method |
---|---|---|---|
Deflection Temperature Under Load | ASTM D648 | ||
0.45 MPa, not annealed | 152 | °C | ASTM D648 |
1.8 MPa, not annealed | 104 | °C | ASTM D648 |
Additional Information |
---|
Testing and measurements were performed at 73 +/-3°F and 50 +/-5% relative humidity unless otherwise noted. |
Injection | Nominal Value | Unit | |
---|---|---|---|
Drying Temperature | 71.1 - 82.2 | °C | |
Drying Time | 2.0 - 4.0 | hr | |
Rear Temperature | 221 - 238 | °C | |
Middle Temperature | 227 - 243 | °C | |
Front Temperature | 232 - 260 | °C | |
Nozzle Temperature | 232 - 260 | °C | |
Processing (Melt) Temp | 221 - 238 | °C | |
Mold Temperature | 37.8 - 65.6 | °C | |
Injection Rate | Slow-Moderate | ||
Back Pressure | 0.138 - 0.345 | MPa | |
Cushion | 5.08 - 12.7 | mm |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
Maxxam™ PP5120 A1 | PolyOne Corporation | PP Homopolymer | Maxxam™ |
THERMOLAST® K TP8VCZ (Series: AD1/CS) | KRAIBURG TPE | TPE | THERMOLAST® K |
Evoprene™ COGEE 628 | AlphaGary | SEBS | Evoprene™ COGEE |
INELEC PEICF20 | Infinity LTL Engineered Compounds | PEI | INELEC |
Sylvin 8200-70 Grey 9539 | Sylvin Technologies Incorporated | PVC, Unspecified | Sylvin |