K-Guard HFFR 771 is a Polyolefin material. It is available in Africa & Middle East.

Important attributes of K-Guard HFFR 771 are:
  • RoHS Compliant
  • Flame Retardant
  • Corrosion Resistant
  • Halogen Free
  • Non-Toxic

Typical application of K-Guard HFFR 771: Wire & Cable
General Information
Additive
  • Flame Retardant
Features
  • Flame Retardant
  • Good Corrosion Resistance
  • Halogen Free
  • Non-Toxic
Uses
  • Wire & Cable Applications
RoHS Compliance
  • RoHS Compliant
PhysicalNominal ValueUnitTest Method
Specific Gravity 1.51g/cm³ASTM D792
Melt Mass-Flow Rate (MFR) (160°C/21.6 kg)5.0g/10 minASTM D1238
HardnessNominal ValueUnitTest Method
Durometer Hardness (Shore D)48ASTM D2240
MechanicalNominal ValueUnitTest Method
Flexural Modulus - 2% Secant 300MPaASTM D790
ElastomersNominal ValueUnitTest Method
Tensile Strength 1(Yield)10.8MPaASTM D412
Tensile Elongation 2(Break)210%ASTM D412
AgingNominal ValueUnitTest Method
Change in Tensile Strength in Air (100°C, 168 hr)12%ASTM D573
Change in Ultimate Elongation in Air (100°C, 168 hr)-22%ASTM D573
Change in Tensile Strength (60°C, 168 hr, in IRM 902 Oil)-11%ASTM D471
ThermalNominal ValueUnitTest Method
Brittleness Temperature -48.0°CASTM D746
ElectricalNominal ValueUnitTest Method
Insulation Resistance 35500Mohms/1000 ftASTM D470
Insulation Resistance Constant - K-Value 419000ASTM D470
FlammabilityNominal ValueUnitTest Method
Heat Release ASTM E1354
    Average 84kW/m²
    Peak 128kW/m²
Additional InformationNominal ValueUnitTest Method
Hot Knife Test (90°C) 5PassIEC 540
Specific Extinction Area 216000m²/kgASTM E1354
Time to Ignition 2.8minASTM E1354
FlammabilityNominal ValueUnitTest Method
Oxygen Index 34%ASTM D2863
Note Message
1 .510 mm/min
2 .510 mm/min
3 .Immersed in water for 16 hrs
4 .Immersed in water for 16 hrs
5 .4 hrs, % penetration, Clause 8
Resin Grade Manufacturer Category Trademark
Trithene® TS 7006 Petroquimica Triunfo LDPE Trithene®
FRblend® PP-1303 Colour Image Plastic Compound Sdn. Bhd. (CIPC) PP, Unspecified FRblend®
Hifax TRC 412P LyondellBasell Industries PP Alloy Hifax
IPC PP 4840H-C International Polymers Corporation PP Homopolymer IPC PP
Latistat 36/MR-04 LATI S.p.A. ABS Latistat