TECHNYL® C 216 V45 Natural is a polyamide 6, reinforced with 45% of glass fibre, for injection moulding. This grade has been optimized to have good impact strength, a nice surface aspect and being easy to paint. |
General Information | |
---|---|
Filler / Reinforcement |
|
Features |
|
Uses |
|
Agency Ratings |
|
RoHS Compliance |
|
Appearance |
|
Forms |
|
Processing Method |
|
Resin ID (ISO 1043) |
|
Physical | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Density | 1.51 | -- | g/cm³ | ISO 1183/A |
Water Absorption (23°C, 24 hr) | 0.80 | -- | % | ISO 62 |
Mechanical | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Tensile Modulus (23°C) | 13000 | 8300 | MPa | ISO 527-2/1A |
Tensile Stress (Break, 23°C) | 190 | 145 | MPa | ISO 527-2/1A |
Tensile Strain (Break, 23°C) | 2.5 | -- | % | ISO 527-2 |
Impact | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Charpy Notched Impact Strength (23°C) | 13 | 26 | kJ/m² | ISO 179/1eA |
Charpy Unnotched Impact Strength (23°C) | 90 | -- | kJ/m² | ISO 179/1eU |
Thermal | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Heat Deflection Temperature (1.8 MPa, Unannealed) | 210 | -- | °C | ISO 75-2/Af |
Melting Temperature | 222 | -- | °C | ISO 11357-3 |
Injection | Dry | Unit | |
---|---|---|---|
Drying Temperature | 80 | °C | |
Suggested Max Moisture | 0.20 | % | |
Rear Temperature | 235 - 240 | °C | |
Middle Temperature | 240 - 250 | °C | |
Front Temperature | 250 - 260 | °C | |
Mold Temperature | 60 - 90 | °C |
Injection instructions |
---|
The material is supplied in airtight bags, ready for use. In case that the virgin material has absorbed moisture, it must be dried with a dehumidified air drying equipment, dew point mini -20°C. Recommended time 2-4hInjection Advice: For reinforced polyamide, Solvay recommends the use of steel with a high content of Carbon and purified for polishing to avoid or limit the abrasion. For example: X38CrMoV5-1 (EN Norm) - 1.2367 /1.2343 (DIN Norm) or X160CrMoV12 (EN Norm) - 1.2601 /1.2379 (DIN Norm). For Mould Temperature, in the case of parts where the surface roughness is required we can recommend a temperature of 90°C to 120°C with an optimum at 105°C. |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
TROSIFOL® VG FR | Kuraray Co., Ltd. | PVB | TROSIFOL® |
Alloy Exchange Reprocessed ABS001 | Alloy Exchange, Inc. | ABS | Alloy Exchange Reprocessed |
Excelprene® GFE-1810 | S&E Specialty Polymers, LLC | PVC+NBR | Excelprene® |
POLYelast TPE ZC100 D40 | Polykemi AB | SEBS | POLYelast |
THERMOLAST® K TF8ADN (Series: FC/AD1/PS) | KRAIBURG TPE | TPE | THERMOLAST® K |