| Category: | SEBS , Styrene Ethylene Butylene Styrene Block Copolymer |
| Manufacturer: | RTP Company |
| Trademark: | RTP |
| Fillers: | - |
| Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
| Delivery Terms | FOB, CIF, DAP, DAT, DDP |
| PDF: | 9R1B3Y_RTP-2700-S-60A-MD-NATURAL.pdf |
| PRICE: | Order Products email sales@su-jiao.com |
| Message |
|---|
| ISO 10993 Tested |
| General Information | |
|---|---|
| Agency Ratings |
|
| RoHS Compliance |
|
| Processing Method |
|
| Physical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Specific Gravity | 0.890 | g/cm³ | ASTM D792 |
| Molding Shrinkage - Flow (3.20 mm) | 1.6 to 2.1 | % | ASTM D955 |
| Hardness | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Durometer Hardness (Shore A, 10 sec) | 60 | ASTM D2240 |
| Elastomers | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Tensile Strength 1(Break, 3.20 mm) | 8.27 | MPa | ASTM D412 |
| Tensile Elongation 2(Break) | 700 | % | ASTM D412 |
| Tear Strength 3 | 35.0 | kN/m | ASTM D624 |
| Compression Set 4 | ASTM D395B | ||
| 23°C, 22 hr | 21 | % | |
| 70°C, 22 hr | 46 | % |
| Injection | Nominal Value | Unit | |
|---|---|---|---|
| Drying Temperature | 76.7 | °C | |
| Drying Time | 2.0 | hr | |
| Processing (Melt) Temp | 177 to 204 | °C | |
| Mold Temperature | 15.6 to 37.8 | °C |
| Note Message | |
|---|---|
| 1 . | Die C, 500 mm/min |
| 2 . | 500 mm/min |
| 3 . | Die C |
| 4 . | Type 2 |
| Resin Grade | Manufacturer | Category | Trademark |
|---|---|---|---|
| Andur 3300 AS/Curative | Anderson Development Company | PUR-TDI | Andur |
| Eraclene® SB 60 | Versalis S.p.A. | HDPE | Eraclene® |
| Latimass 53/11-02 D030 | LATI S.p.A. | PP Homopolymer | Latimass |
| LUVOCOM® 1850-8710 | Lehmann & Voss & Co. | PBT | LUVOCOM® |
| POLYCOMPO PE 2022L | POLYCOMPO Co.,Ltd. | LLDPE | POLYCOMPO PE |