| Category: | PUR-Ether/TDI , Polyurethane (Polyether, TDI) |
| Manufacturer: | Anderson Development Company |
| Trademark: | Andur |
| Fillers: | - |
| Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
| Delivery Terms | FOB, CIF, DAP, DAT, DDP |
| PDF: | 9Kp0Zb_Andur-8-AP-Curene-442.pdf |
| PRICE: | Order Products email sales@su-jiao.com |
| Message |
|---|
| All properties based on Andur® 8-AP cured with Curene® 442 |
| General Information | |
|---|---|
| Forms |
|
| Processing Method |
|
| Hardness | Nominal Value | Test Method | |
|---|---|---|---|
| Durometer Hardness (Shore A) | 80 | ASTM D2240 |
| Mechanical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Tensile Strength | 45.5 | MPa | ASTM D638 |
| Tensile Elongation (Break) | 550 | % | ASTM D638 |
| Elastomers | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Tensile Stress | ASTM D412 | ||
| 100% strain | 4.07 | MPa | ASTM D412 |
| 300% strain | 7.93 | MPa | ASTM D412 |
| Tear Strength 1 | 84.1 | kN/m | ASTM D624 |
| Compression Set | 27 | % | ASTM D395 |
| Thermoset | Nominal Value | Unit | |
|---|---|---|---|
| Pot Life | 16 - 17 | min | |
| Demold Time | 30 - 35 | min |
| Additional Information |
|---|
| Hardness, Shore A: 80-82Curene® 442 Temperature, °F: 240-250Prepolymer Temperature, °F: 212-220 |
| Note Message | |
|---|---|
| 1 . | C mould |
| Resin Grade | Manufacturer | Category | Trademark |
|---|---|---|---|
| Mirakutoran® TPU E885PFAB | Japan Mirakutoran Inc. | TPU Alloy | Mirakutoran® TPU |
| Styropor® F 415 E | BASF Corporation | PS (EPS) | Styropor® |
| Abstron AN450EVM | Bhansali Engineering Polymers Limited | ABS | Abstron |
| Hiprolon® 70 HVN | Arkema | Nylon 610 | Hiprolon® |
| Hostacom CR 1171 G1 | LyondellBasell Industries | PP Impact Copolymer | Hostacom |