| Category: | TPV , Thermoplastic Vulcanizate |
| Manufacturer: | Teknor Apex Company |
| Trademark: | Sarlink® TPV |
| Fillers: | - |
| Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
| Delivery Terms | FOB, CIF, DAP, DAT, DDP |
| PDF: | 9CoRyx_Sarlink-TPV-2573.pdf |
| PRICE: | Order Products email sales@su-jiao.com |
| Message |
|---|
|
Sarlink®TPV 2573 is a thermoplastic vulcanized rubber (TPV) material,. This product is available in North America, Africa and the Middle East, Latin America, Europe or Asia Pacific. The processing method is extrusion or injection molding. Typical application areas include:
|
| General Information | |
|---|---|
| Uses |
|
| Appearance |
|
| Forms |
|
| Processing Method |
|
| Physical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Specific Gravity | 0.928 | g/cm³ | ASTM D792 |
| Melt Mass-Flow Rate (MFR) (230°C/2.16 kg) | 0.60 | g/10 min | ASTM D1238 |
| Hardness | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Durometer Hardness | ASTM D2240 | ||
| Shaw A | 76 | ASTM D2240 | |
| Shaw A, 5 seconds | 73 | ASTM D2240 |
| Elastomers | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Tensile Strength (Break) | 7.17 | MPa | ASTM D412 |
| Tensile Elongation (Break) | 320 | % | ASTM D412 |
| Compression Set | ASTM D395B | ||
| 22°C, 22 hr | 27 | % | ASTM D395B |
| 70°C, 22 hr | 37 | % | ASTM D395B |
| Thermal | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Brittleness Temperature | < -60.0 | °C | ASTM D746 |
| Injection | Nominal Value | Unit | |
|---|---|---|---|
| Rear Temperature | 173 - 213 | °C | |
| Middle Temperature | 179 - 219 | °C | |
| Front Temperature | 184 - 224 | °C | |
| Nozzle Temperature | 190 - 230 | °C | |
| Processing (Melt) Temp | 190 - 230 | °C | |
| Mold Temperature | 35.0 - 60.0 | °C | |
| Injection Pressure | 1.38 - 6.89 | MPa | |
| Injection Rate | Fast | ||
| Back Pressure | 0.172 - 0.862 | MPa | |
| Screw Speed | 50 - 120 | rpm | |
| Cushion | 3.81 - 25.4 | mm |
| Extrusion | Nominal Value | Unit | |
|---|---|---|---|
| Cylinder Zone 1 Temp. | 166 - 204 | °C | |
| Cylinder Zone 2 Temp. | 171 - 210 | °C | |
| Cylinder Zone 3 Temp. | 177 - 216 | °C | |
| Cylinder Zone 5 Temp. | 182 - 221 | °C | |
| Die Temperature | 190 - 227 | °C |
| Extrusion instructions |
|---|
| 螺杆转速30 - 100 rpm |
| Resin Grade | Manufacturer | Category | Trademark |
|---|---|---|---|
| RTP 1207-70A | RTP Company | TPU-Polyester | RTP |
| AMTOPP TT18 | Inteplast Group | PP, Unspecified | AMTOPP |
| Dugdale PVC Rigid Extrusion White Compound | Dugdale Plc | PVC, Rigid | Dugdale PVC |
| Karina BLACK PVC COMPOUND -E 70900-48/ 1-E-AC | Karina Ind. e Com. de Plásticos Ltda | PVC, Unspecified | Karina |
| Sylvin 7833-85C Natural | Sylvin Technologies Incorporated | PVC, Unspecified | Sylvin |