| Category: | PP, Unspecified , Polypropylene |
| Manufacturer: | EMAS Plastik San.Tic.AS. |
| Trademark: | EMOPLEN® |
| Fillers: | - |
| Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
| Delivery Terms | FOB, CIF, DAP, DAT, DDP |
| PDF: | 9AraM9_EMOPLEN-A-1208-T2.pdf |
| PRICE: | Order Products email sales@su-jiao.com |
| Message |
|---|
| Polypropylene %20 talcum filled |
| General Information | |
|---|---|
| Filler / Reinforcement |
|
| Uses |
|
| Physical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Density | 1.00 to 1.05 | g/cm³ | ISO 1183 |
| Melt Mass-Flow Rate (MFR) (230°C/2.16 kg) | 10 to 14 | g/10 min | ISO 1133 |
| Molding Shrinkage | 0.90 to 1.0 | % |
| Hardness | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Shore Hardness (Shore D) | 60 to 65 | ISO 868 |
| Mechanical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Tensile Modulus | 2500 to 3500 | MPa | ISO 527-2 |
| Tensile Stress (Yield) | 25.0 to 35.0 | MPa | ISO 527-2 |
| Tensile Strain (Break) | > 6.0 | % | ISO 527-2 |
| Impact | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Notched Izod Impact Strength | > 8.0 | kJ/m² | ISO 180/1A |
| Thermal | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Heat Deflection Temperature (1.8 MPa, Unannealed) | 105 | °C | ISO 75-2/A |
| Vicat Softening Temperature | 95.0 | °C | ISO 306/B |
| Melting Temperature (DSC) | 160 | °C | ISO 3146 |
| Resin Grade | Manufacturer | Category | Trademark |
|---|---|---|---|
| Premi-Glas® 2103-22 CR-SX-HT | Premix, Inc. | TS, Unspecified | Premi-Glas® |
| RTP 6011-65A | RTP Company | TPE | RTP |
| Primefin E535/30GC | Lucent Polymers, Inc. | PP, Unspecified | Primefin |
| NAXALOY® 770-BK272 | MRC Polymers, Inc. | PC+ABS | NAXALOY® |
| BR® 6700-1 | Cytec Industries Inc. | Epoxy | BR® |