| Physical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Density | 1.45 | g/cm³ | ISO 1183 |
| shrinkage- Flow (3.00 mm) | 0.30 - 0.70 | % | ISO 294-4 |
| Water Absorption (Equilibrium, 23°C, 50% RH) | 0.50 | % | ISO 62 |
| Mechanical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Tensile Stress | 210 | MPa | ISO 527-2 |
| Tensile Strain (Break) | 2.2 | % | ISO 527-2 |
| Flexural Modulus | 10100 | MPa | ISO 178 |
| Flexural Stress | 300 | MPa | ISO 178 |
| Impact | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Charpy Notched Impact Strength (23°C) | 11 | kJ/m² | ISO 179/1eA |
| Thermal | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Heat Deflection Temperature (1.8 MPa, Unannealed) | 275 | °C | ISO 75-2/A |
| Melting Temperature 1 | 310 | °C | ISO 11357-3 |
| CLTE - Flow | 2.2E-5 - 5.3E-5 | cm/cm/°C | ISO 11359-2 |
| Electrical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Surface Resistivity | 1.0E+16 | ohms | IEC 60093 |
| Volume Resistivity | 1.0E+15 | ohms·cm | IEC 60093 |
| Dielectric Strength | 28 | kV/mm | IEC 60243-1 |
| Relative Permittivity (1 MHz) | 4.20 | IEC 60250 | |
| Dissipation Factor (1 MHz) | 2.0E-3 | IEC 60250 |
| Flammability | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Flame Rating (0.8 mm) | HB | UL 94 |
| Injection | Nominal Value | Unit | |
|---|---|---|---|
| Drying Temperature | |||
| Dry Air Dryer, A | 90 | °C | |
| Dry Air Dryer, B | 120 | °C | |
| Drying Time | |||
| Dry Air Dryer, A | 8.0 | hr | |
| Dry Air Dryer, B | 4.0 | hr | |
| Suggested Max Moisture | 0.10 | % | |
| Hopper Temperature | 60 - 80 | °C | |
| Rear Temperature | 310 - 330 | °C | |
| Middle Temperature | 310 - 335 | °C | |
| Front Temperature | 315 - 340 | °C | |
| Nozzle Temperature | 320 - 340 | °C | |
| Mold Temperature | 130 - 150 | °C |
| Note Message | |
|---|---|
| 1 . | 10°C/min |
| Resin Grade | Manufacturer | Category | Trademark |
|---|---|---|---|
| RTP 4082 A | RTP Company | PPA | RTP |
| Rhelon G1533HU-01 | RheTech, Inc. | Nylon 6 | Rhelon |
| SureSpec HP-040 | Genesis Polymers | PP, HMS | SureSpec |
| Formolene® 6501A | Formosa Plastics Corporation, U.S.A. | PP Impact Copolymer | Formolene® |
| KRATON® D2104 DI-N | Kraton Polymers LLC | SBS | KRATON® |