Category: | TPU-Polyester , Thermoplastic Polyurethane Elastomer (Polyester) |
Manufacturer: | Huntsman Corporation |
Trademark: | IROGRAN® |
Fillers: | - |
Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
Delivery Terms | FOB, CIF, DAP, DAT, DDP |
PDF: | 90gVmt_IROGRAN-A-92-H-4656.pdf ![]() |
PRICE: | Order Products email sales@su-jiao.com |
Message |
---|
IROGRAN A 92 H 4656 is a thermoplastic polyester-polyurethane for injection moulding applications. Additional characteristics of the product are short cycle times, good melt flow and easy demolding. PERFORMANCE FEATURES
APPLICATIONS For the production of technical parts, wheels and rollers, cover plates, coupling halfs, conveyor rollers. |
General Information | |
---|---|
Features |
|
Uses |
|
RoHS Compliance |
|
Forms |
|
Processing Method |
|
Physical | Nominal Value | Unit | Test Method |
---|---|---|---|
Specific Gravity | 1.21 | g/cm³ | |
Molding Shrinkage | |||
Flow : Injection Molded | 0.60 | % | ASTM D955 |
-- 1 | 0.40 | % |
Hardness | Nominal Value | Unit | Test Method |
---|---|---|---|
Durometer Hardness | |||
Shore A, Injection Molded | 85 | ASTM D2240 | |
Shore D, Injection Molded | 34 | ASTM D2240 | |
Shore A, Injection Molded | 92 | ISO 868 | |
Shore D, Injection Molded | 40 | ISO 868 |
Mechanical | Nominal Value | Unit | Test Method |
---|---|---|---|
Abrasion 2 | 30 | mm³ | ISO 4649 |
Elastomers | Nominal Value | Unit | Test Method |
---|---|---|---|
Tensile Stress 3 | |||
100% Strain | 4.90 | MPa | ASTM D412 |
100% Strain | 9.00 | MPa | DIN 53504 |
300% Strain | 11.0 | MPa | ASTM D412 |
300% Strain | 21.0 | MPa | DIN 53504 |
Tensile Strength 4 | |||
Break | 36.0 | MPa | ASTM D412 |
Break | 45.0 | MPa | DIN 53504 |
Tensile Elongation 5 | |||
Break | 750 | % | ASTM D412 |
Break | 550 | % | DIN 53504 |
Tear Strength 6 | |||
-- | 99.8 | kN/m | ASTM D624 |
-- | 120 | kN/m | ISO 34-1 |
Compression Set 7 | |||
23°C, 24 hr | 25 | % | ASTM D395, ISO 815 |
70°C, 24 hr | 40 | % | ASTM D395 |
73°C, 24 hr | 40 | % | ISO 815 |
Injection | Nominal Value | Unit | |
---|---|---|---|
Drying Temperature | |||
-- | 100 to 110 | °C | |
Hot Air Dryer | 80.0 to 90.0 | °C | |
Drying Time | |||
-- | 3.0 | hr | |
Hot Air Dryer | 3.0 | hr | |
Dew Point | -30.0 | °C | |
Rear Temperature | 175 to 195 | °C | |
Middle Temperature | 175 to 195 | °C | |
Front Temperature | 175 to 195 | °C | |
Nozzle Temperature | 180 to 200 | °C | |
Processing (Melt) Temp | 170 to 195 | °C | |
Mold Temperature | 20.0 to 70.0 | °C |
Extrusion | Nominal Value | Unit | |
---|---|---|---|
Drying Temperature | 100 to 110 | °C | |
Drying Time | 3.0 | hr | |
Hopper Temperature | 25.0 to 40.0 | °C | |
Cylinder Zone 1 Temp. | 165 to 190 | °C | |
Cylinder Zone 2 Temp. | 165 to 190 | °C | |
Cylinder Zone 3 Temp. | 165 to 190 | °C | |
Cylinder Zone 4 Temp. | 165 to 190 | °C | |
Cylinder Zone 5 Temp. | 165 to 190 | °C | |
Adapter Temperature | 175 to 195 | °C | |
Die Temperature | 175 to 200 | °C |
Note Message | |
---|---|
1 . | Injection Molded |
2 . | Injection Molded |
3 . | Injection Molded |
4 . | Injection Molded |
5 . | Injection Molded |
6 . | Injection Molded |
7 . | Injection Molded |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
POLYplex PMMA 700 | Polykemi AB | Acrylic (PMMA) | POLYplex |
Braskem PP TR3350CW2 | Braskem America Inc. | PP Random Copolymer | Braskem PP |
Greene FKM 761 | Greene, Tweed & Co. | Fluorelastomer | Greene FKM |
KMI PC 101HMB | KMI Group Inc. | PC | KMI PC |
Lion Idemitsu Composites PPS C-140SF | Lion Idemitsu Composites Co., Ltd. | PPS | Lion Idemitsu Composites PPS |