Category: | Nylon 6 Alloy , Polyamide 6 Alloy |
Manufacturer: | Arkema |
Trademark: | Orgalloy® |
Fillers: | - |
Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
Delivery Terms | FOB, CIF, DAP, DAT, DDP |
PDF: | 7zfu04_Orgalloy-LE-60HM.pdf ![]() |
PRICE: | Order Products email sales@su-jiao.com |
Message |
---|
Orgalloy® LE 60HM is a Polyamide 6 Alloy (Nylon 6 Alloy) product. It can be processed by blow molding, calendering, extrusion, film extrusion, injection molding, profile extrusion, resin transfer molding, sheet extrusion, or thermoforming and is available in Africa & Middle East, Asia Pacific, Europe, Latin America, or North America. Characteristics include:
|
General Information | |
---|---|
Features |
|
Forms |
|
Processing Method |
|
Multi-Point Data |
|
Physical | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Density | 1050 | 1050 | kg/m³ | ISO 1183 1 |
Melt volume-flow rate (235°C/2.16 kg) | 1.00 | -- | cm³/10min | ISO 1133 2 |
Water Absorption | ISO 62 3 | |||
Saturation | 6.4 | -- | % | |
Equilibrium | 1.8 | -- | % |
Mechanical | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Tensile modulus | -- | 1550 | MPa | ISO 527-2 4 |
Tensile Stress (Yield) | -- | 39.0 | MPa | ISO 527-2 5 |
Tensile Strain (Yield) | -- | 5.0 | % | ISO 527-2 6 |
Nominal strain at break | -- | > 50 | % | ISO 527-2 7 |
Tensile Creep Modulus | ISO 899-1 8 | |||
1 hr | -- | 1350 | MPa | |
1000 hr | -- | 620 | MPa |
Thermal | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Melting Temperature 9 | 220 | -- | °C | ISO 11357-3 10 |
Electrical | Dry | Conditioned | Test Method | |
---|---|---|---|---|
Comparative tracking index | -- | 600 | IEC 60112 11 |
Flammability | Dry | Conditioned | Test Method | |
---|---|---|---|---|
Burning Behav. at 1.6mm nom. thickn. (1.60 mm) | HB | -- | ISO 1210 12 | |
Burning Behav. at thickness h (3.20 mm) | HB | -- | ISO 1210 13 |
Note Message | |
---|---|
1 . | Tested in accordance with ISO 10350. 23°C/50%r.h. unless otherwise noted. |
2 . | Tested in accordance with ISO 10350. 23°C/50%r.h. unless otherwise noted. |
3 . | Tested in accordance with ISO 10350. 23°C/50%r.h. unless otherwise noted. |
4 . | Tested in accordance with ISO 10350. 23°C/50%r.h. unless otherwise noted. |
5 . | Tested in accordance with ISO 10350. 23°C/50%r.h. unless otherwise noted. |
6 . | Tested in accordance with ISO 10350. 23°C/50%r.h. unless otherwise noted. |
7 . | Tested in accordance with ISO 10350. 23°C/50%r.h. unless otherwise noted. |
8 . | Tested in accordance with ISO 10350. 23°C/50%r.h. unless otherwise noted. |
9 . | 10 °C/min |
10 . | Tested in accordance with ISO 10350. 23°C/50%r.h. unless otherwise noted. |
11 . | Tested in accordance with ISO 10350. 23°C/50%r.h. unless otherwise noted. |
12 . | Tested in accordance with ISO 10350. 23°C/50%r.h. unless otherwise noted. |
13 . | Tested in accordance with ISO 10350. 23°C/50%r.h. unless otherwise noted. |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
PRIMALLOY® B1932 | Mitsubishi Chemical Performance Polymers, Inc. | TPE | PRIMALLOY® |
Sinelec CCB6285 | Teknor Apex Asia Pacific PTE. LTD. | PS (Specialty) | Sinelec |
apilon 52® A7505 | API SpA | TPU-Polyester | apilon 52® |
Chemical Resources LD38921 | Chemical Resources, Inc. | LDPE | Chemical Resources |
Innova N 1841 | Innova SA | PS (GPPS) | Innova |