| Category: | LLDPE , Linear Low Density Polyethylene |
| Manufacturer: | Westlake Chemical Corporation |
| Trademark: | HIFOR Xtreme® |
| Fillers: | - |
| Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
| Delivery Terms | FOB, CIF, DAP, DAT, DDP |
| PDF: | 6UBxLd_HIFORXtremeSC74871.pdf |
| PRICE: | Order Products email sales@su-jiao.com |
| Message |
|---|
|
WESTLAKE HIFOR Xtreme SC74871 is a Hexene LLDPE designed for cast film extrusion. This material is stabilized for cast film extrusion, and contains no slip, anti-block, or process aid. Application/Uses
|
| General Information | |
|---|---|
| Features |
|
| Uses |
|
| Agency Ratings |
|
| Processing Method |
|
| Physical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Density | 0.919 | g/cm³ | ASTM D1505 |
| Melt Mass-Flow Rate (MFR) (190°C/2.16 kg) | 2.0 | g/10 min | ASTM D1238 |
| Films | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Film Thickness - Tested | 20 | µm | |
| secant modulus | ASTM D882 | ||
| 1% secant, MD : 20 µm, cast film | 138 | MPa | ASTM D882 |
| 1% secant, TD : 20 µm, cast film | 152 | MPa | ASTM D882 |
| Tensile Strength | ASTM D882 | ||
| MD : Fracture, 20 µm, extruded film | 51.7 | MPa | ASTM D882 |
| TD : Fracture, 20 µm, extruded film | 33.1 | MPa | ASTM D882 |
| Tensile Elongation | ASTM D882 | ||
| MD : Fracture, 20 µm, extruded film | 500 | % | ASTM D882 |
| TD : Fracture, 20 µm, extruded film | 850 | % | ASTM D882 |
| Dart Drop Impact (20 µm, Cast Film) | 85 | g | ASTM D1709 |
| Optical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Haze (20.3 µm, cast film) | 2.5 | % | ASTM D1003 |
| Resin Grade | Manufacturer | Category | Trademark |
|---|---|---|---|
| Radilon® AGV 40 Black | Radici Plastics | Nylon 66 | Radilon® |
| Nypol® PA A3 G20 V10 PRTA010 NR302 MSP | Petropol Industry and Trade of Polymers LTDA | Nylon 66 | Nypol® PA |
| CERTENE™ HPB-0345 | Muehlstein | HDPE | CERTENE™ |
| G-Lex B63A003 | Gas Authority of India Limited | HDPE | G-Lex |
| POLYabs HD2 | Polykemi AB | ABS | POLYabs |