LDPE FE 8000 is a low density polyethylene produced by a high pressure autoclave process. This grade is particularly suitable for transparent thin film. LDPE FE 8000 is suited to many applications in the field of consumer, industrial, food or hygiene packaging such as collation shrink, lamination and coextrusion film. |
General Information | |
---|---|
Uses |
|
Agency Ratings |
|
Forms |
|
Processing Method |
|
Multi-Point Data |
|
Physical | Nominal Value | Unit | Test Method |
---|---|---|---|
Density | |||
-- | 0.924 | g/cm³ | ISO 1183 |
-- | 924 | kg/m³ | ISO 1183 1 |
Melt Mass-Flow Rate (MFR) (190°C/2.16 kg) | 0.80 | g/10 min | ISO 1133 |
Melt volume-flow rate (190°C/2.16 kg) | 1.00 | cm³/10min | ISO 1133 2 |
Water Absorption (Saturation) | 0.010 | % | ISO 62 3 |
Mechanical | Nominal Value | Unit | Test Method |
---|---|---|---|
Tensile Modulus | 240 | MPa | ISO 527-2 4 |
Tensile Stress (Yield) | 12.0 | MPa | ISO 527-2 5 |
Tensile Strain (Yield) | 15 | % | ISO 527-2 6 |
Tensile Elongation at Break | > 50 | % | ISO 527-2 7 |
Films | Nominal Value | Unit | Test Method |
---|---|---|---|
Tensile Stress | ISO 527-3 | ||
MD : Yield, 40 µm, blown film | 12.0 | MPa | ISO 527-3 |
TD : Yield, 40 µm, blown film | 12.0 | MPa | ISO 527-3 |
MD : Broken, 40 µm, blown film | 27.0 | MPa | ISO 527-3 |
TD : Broken, 40 µm, blown film | 23.0 | MPa | ISO 527-3 |
Tensile Elongation | ISO 527-3 | ||
MD : Broken, 40 µm, blown film | 370 | % | ISO 527-3 |
TD : Broken, 40 µm, blown film | 570 | % | ISO 527-3 |
Dart Drop Impact (40 µm, Blown Film) | 120 | g | ISO 7765-1 |
Thermal | Nominal Value | Unit | Test Method |
---|---|---|---|
Heat Deflection Temperature (1.8 MPa) | 41.0 | °C | ISO 75-2 8 |
Vicat Softening Temperature | |||
-- | 99.0 | °C | ISO 306 |
50°C/h, B (50N) | 98.0 | °C | ISO 306 9 |
Melting Temperature (DSC) | |||
-- | 111 | °C | ISO 3146 |
-- 10 | 114 | °C | ISO 11357-3 11 |
CLTE - Flow | 1.8E-4 | cm/cm/°C | ISO 11359-2 12 |
Electrical | Nominal Value | Unit | Test Method |
---|---|---|---|
Surface Resistivity | 1.0E+14 | ohms | IEC 60093 13 |
Volume Resistivity | > 1.0E+13 | ohms·m | IEC 60093 14 |
Relative Permittivity (100 Hz) | 2.00 | IEC 60250 15 | |
Dissipation Factor | IEC 60250 16 | ||
100 Hz | 2.0E-4 | IEC 60250 | |
1 MHz | 2.0E-4 | IEC 60250 | |
Comparative Tracking Index | 600 | IEC 60112 17 |
Flammability | Nominal Value | Unit | Test Method |
---|---|---|---|
Burning Behav. at 1.6mm nom. thickn. (1.60 mm) | HB | ISO 1210 18 | |
Oxygen Index | 18 | % | ISO 4589-2 19 |
Additional Information |
---|
The value listed as Melting Temperature, ISO 3146, was tested in accordance with ISO 11357.Elmendorf, ISO 6383-2, MD, Blown Film, 40 µm: 53 N/mmElmendorf, ISO 6383-2, TD, Blown Film, 40 µm: 47 N/mmHaze, ISO 14782, Blown Film, 40 µm: 11% |
Extrusion | Nominal Value | Unit | |
---|---|---|---|
Cylinder Zone 1 Temp. | 160 - 200 | °C | |
Cylinder Zone 2 Temp. | 160 - 200 | °C | |
Cylinder Zone 3 Temp. | 160 - 200 | °C | |
Cylinder Zone 4 Temp. | 160 - 200 | °C | |
Cylinder Zone 5 Temp. | 160 - 200 | °C |
Note Message | |
---|---|
1 . | ??????,?? ISO 10350 ??? 23°C/50%r.h. ??? |
2 . | ??????,?? ISO 10350 ??? 23°C/50%r.h. ??? |
3 . | ??????,?? ISO 10350 ??? 23°C/50%r.h. ??? |
4 . | ??????,?? ISO 10350 ??? 23°C/50%r.h. ??? |
5 . | ??????,?? ISO 10350 ??? 23°C/50%r.h. ??? |
6 . | ??????,?? ISO 10350 ??? 23°C/50%r.h. ??? |
7 . | ??????,?? ISO 10350 ??? 23°C/50%r.h. ??? |
8 . | ??????,?? ISO 10350 ??? 23°C/50%r.h. ??? |
9 . | ??????,?? ISO 10350 ??? 23°C/50%r.h. ??? |
10 . | 10 °C/min |
11 . | ??????,?? ISO 10350 ??? 23°C/50%r.h. ??? |
12 . | ??????,?? ISO 10350 ??? 23°C/50%r.h. ??? |
13 . | ??????,?? ISO 10350 ??? 23°C/50%r.h. ??? |
14 . | ??????,?? ISO 10350 ??? 23°C/50%r.h. ??? |
15 . | ??????,?? ISO 10350 ??? 23°C/50%r.h. ??? |
16 . | ??????,?? ISO 10350 ??? 23°C/50%r.h. ??? |
17 . | ??????,?? ISO 10350 ??? 23°C/50%r.h. ??? |
18 . | ??????,?? ISO 10350 ??? 23°C/50%r.h. ??? |
19 . | ??????,?? ISO 10350 ??? 23°C/50%r.h. ??? |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
Medalist® MD-50288 | Teknor Apex Company | TPE | Medalist® |
Tenite™ Butyrate 485E3720023 Clear, Trsp | Eastman Chemical Company | CAB | Tenite™ Butyrate |
Sylvin 5174-83 Natural | Sylvin Technologies Incorporated | PVC, Unspecified | Sylvin |
ASI POLYETHYLENE CP 851 | A. Schulman Inc. | LDPE | ASI POLYETHYLENE |
Fiberfil® PP-60/TC/20 | Fiberfil® Engineered Plastics Inc. | PP Homopolymer | Fiberfil® |