Category: | Nylon 612 , Polyamide 612 |
Manufacturer: | Mazzaferro Indústria e Comércio de Polímeros e Fibras Ltda. |
Trademark: | MAZMID D |
Fillers: | - |
Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
Delivery Terms | FOB, CIF, DAP, DAT, DDP |
PDF: | 69Iu0S_MAZMID-D-300-FV13.pdf ![]() |
PRICE: | Order Products email sales@su-jiao.com |
Message |
---|
MAZMID D 300 FV13 is a Polyamide 612 (Nylon 612) product filled with 13% glass fiber. It can be processed by injection molding and is available in Latin America. Typical application: Engineering/Industrial Parts. Characteristics include:
|
General Information | |
---|---|
Filler / Reinforcement |
|
Features |
|
Uses |
|
Appearance |
|
Processing Method |
|
Physical | Nominal Value | Unit | Test Method |
---|---|---|---|
Density | 1.15 | g/cm³ | ISO 1183 |
Water Absorption (23°C, 24 hr) | 0.15 | % | ISO 62 |
Mechanical | Nominal Value | Unit | Test Method |
---|---|---|---|
Tensile Modulus | 3000 | MPa | ISO 527-2 |
Tensile Stress (Yield) | 75.0 | MPa | ISO 527-2 |
Tensile Strain (Break) | 12 | % | ISO 527-2 |
Flexural Modulus | 3500 | MPa | ISO 178 |
Flexural Stress | 85.0 | MPa | ISO 178 |
Impact | Nominal Value | Unit | Test Method |
---|---|---|---|
Notched Izod Impact Strength | ISO 180 | ||
-40°C | 4.5 | kJ/m² | |
23°C | 11 | kJ/m² |
Thermal | Nominal Value | Unit | Test Method |
---|---|---|---|
Heat Deflection Temperature | |||
0.45 MPa, Unannealed | 190 | °C | ISO 75-2/B |
1.8 MPa, Unannealed | 150 | °C | ISO 75-2/A |
Melting Temperature (DSC) | 212 to 215 | °C | ISO 1218 |
Flammability | Nominal Value | Test Method | |
---|---|---|---|
Flame Rating (1.30 mm) | HB | UL 94 |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
BR® 680-3 | Cytec Industries Inc. | PI, TS | BR® |
Evoprene™ GC 5685 | AlphaGary | SEBS | Evoprene™ GC |
Fainplast PVC GS 56/R | Fainplast Compounds S.r.l | PVC, Unspecified | Fainplast PVC |
MAJORIS DFR121R | AD majoris | PP, Unspecified | MAJORIS |
Sumikon® PM-TX250 | SBHPP | Phenolic | Sumikon® |