| Category: | PVC, Unspecified , Polyvinyl Chloride |
| Manufacturer: | Shandong Jining Bolv Chemicals Co.,Ltd |
| Trademark: | Bolv |
| Fillers: | - |
| Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
| Delivery Terms | FOB, CIF, DAP, DAT, DDP |
| PDF: | 5vhqYv_Bolv-PVC.pdf |
| PRICE: | Order Products email sales@su-jiao.com |
| Message |
|---|
| Bolv PVC is a Polyvinyl Chloride material. It is available in Asia Pacific. |
| General Information | |
|---|---|
| Appearance |
|
| Forms |
|
| Physical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Density 1 | < 1.45 | g/cm³ | ASTM D1505 |
| Hardness | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Durometer Hardness 2(Shore A) | < 80 | ASTM D2240 |
| Mechanical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Tensile Strength 3 | > 15.0 | MPa | ASTM D638 |
| Tensile Elongation | ASTM D638 | ||
| Break 4 | > 310 | % | |
| Break | > 180 | % |
| Aging | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Change in Tensile Strength (100°C, 168 hr) | < 20 | % | ASTM D471 |
| Change in Ultimate Elongation (100°C, 168 hr) | < 20 | % | ASTM D471 |
| Thermal | Nominal Value | Unit | |
|---|---|---|---|
| Hot Deformation 5 | < 50 | % | |
| Low Temperature Brittleness 6 | -20 | °C | |
| Thermal Stability 7(200°C) | > 50 | min |
| Additional Information | Nominal Value | Unit | |
|---|---|---|---|
| Weight Loss on Heating 8 | < 23 | g/m² |
| Electrical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Volume Resistivity 9(20°C) | > 1.0E+10 | ohms·cm | ASTM D257 |
| Dielectric Strength 10 | > 18 | kV/mm | ASTM D149 |
| Flammability | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Oxygen Index 11 | > 30 | % | ASTM D2863 |
| Note Message | |
|---|---|
| 1 . | Aged for 168 hr at 100°C |
| 2 . | Aged for 168 hr at 100°C |
| 3 . | Aged for 168 hr at 100°C |
| 4 . | Aged for 168 hr at 100°C |
| 5 . | Aged for 168 hr at 100°C |
| 6 . | Aged for 168 hr at 100°C |
| 7 . | Aged for 168 hr at 100°C |
| 8 . | Aged for 168 hr at 100°C |
| 9 . | Aged for 168 hr at 100°C |
| 10 . | Aged for 168 hr at 100°C |
| 11 . | Aged for 168 hr at 100°C |
| Resin Grade | Manufacturer | Category | Trademark |
|---|---|---|---|
| TEKNIFLEX® PX 12 | Tekni-Films, a div of Tekni-Plex | Film, Copolyester | TEKNIFLEX® |
| Syncure™ V0045G RoHS | PolyOne Corporation | XLPE | Syncure™ |
| VESTAMID® L L2122 | Evonik Industries AG | Nylon 12 | VESTAMID® L |
| Accura® CastPro™ | 3D Systems | Unspecified | Accura® |
| CYCOLAC™ EX58F resin | SABIC Innovative Plastics | ABS | CYCOLAC™ |