Category: | PP, Unspecified , Polypropylene |
Manufacturer: | Putsch Kunststoffe GmbH |
Trademark: | FORMULA P |
Fillers: | - |
Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
Delivery Terms | FOB, CIF, DAP, DAT, DDP |
PDF: | 5vf0Bv_FORMULA-P-ELAN-3003.pdf ![]() |
PRICE: | Order Products email sales@su-jiao.com |
Message |
---|
Polypropylene Elastomer. High impact resistance at low temperatures. |
General Information | |
---|---|
Features |
|
Physical | Nominal Value | Unit | Test Method |
---|---|---|---|
Density | 0.900 | g/cm³ | ISO 1183 |
Melt Mass-Flow Rate (MFR) (230°C/2.16 kg) | 4.0 | g/10 min | ISO 1133 |
Mechanical | Nominal Value | Unit | Test Method |
---|---|---|---|
Tensile Stress | ISO 527-2 | ||
Yield | 18.0 | MPa | ISO 527-2 |
Fracture | 17.0 | MPa | ISO 527-2 |
Tensile Strain (Break) | > 400 | % | ISO 527-2 |
Flexural Modulus | 1000 | MPa | ISO 178 |
Flexural Stress (3.5% Strain) | 37.0 | MPa | ISO 178 |
Impact | Nominal Value | Unit | Test Method |
---|---|---|---|
Notched Izod Impact | ISO 180 | ||
-20°C | 7.0 | kJ/m² | ISO 180 |
23°C | 35 | kJ/m² | ISO 180 |
Thermal | Nominal Value | Unit | Test Method |
---|---|---|---|
Vicat Softening Temperature | 58.0 | °C | ISO 306/B |
Additional Information |
---|
Tensile Strength, ISO 527: 18 MPa |
Injection | Nominal Value | Unit | |
---|---|---|---|
Processing (Melt) Temp | 220 - 240 | °C | |
Mold Temperature | 30.0 - 60.0 | °C |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
XYRON™ 1951J | Asahi Kasei Chemicals Corporation | PPE+PS | XYRON™ |
ADENE GHQAG | A.D. Compound spa | PP Copolymer | ADENE |
Cabofor® 28 GF/20 NATURALE | SO.F.TER. SPA | PC | Cabofor® |
Hanwha Total PP HTB52 | HANWHA TOTAL PETROCHEMICALS Co., Ltd. | PP, Unspecified | Hanwha Total PP |