Category: | SEBS , Styrene Ethylene Butylene Styrene Block Copolymer |
Manufacturer: | Elastron USA, Inc. |
Trademark: | Elastron® G |
Fillers: | - |
Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
Delivery Terms | FOB, CIF, DAP, DAT, DDP |
PDF: | 5RIQ8Y_Elastron-G-G301-A65-N.pdf ![]() |
PRICE: | Order Products email sales@su-jiao.com |
Message |
---|
A soft, colorable SEBS based thermoplastic elastomer (TPE) compound that offers good physical properties and chemical resistance. Bondable to: PP, EVA, PE |
General Information | |
---|---|
Features |
|
RoHS Compliance |
|
Appearance |
|
Forms |
|
Processing Method |
|
Physical | Nominal Value | Unit | Test Method |
---|---|---|---|
Specific Gravity | 0.990 | g/cm³ | ASTM D792 |
Molding Shrinkage | ASTM D955 | ||
Flow | 2.1 | % | |
Across Flow | 1.3 | % |
Hardness | Nominal Value | Unit | Test Method |
---|---|---|---|
Durometer Hardness (Shore A) | 65 | ASTM D2240 |
Mechanical | Nominal Value | Unit | Test Method |
---|---|---|---|
Abrasion | 110 | mm³ | ASTM D1630 |
Additional Information | Nominal Value | Test Method | |
---|---|---|---|
Ozone Resistance - Stressed | No Cracks | ASTM D518 |
Elastomers | Nominal Value | Unit | Test Method |
---|---|---|---|
Tensile Stress | ASTM D412 | ||
100% Strain | 2.10 | MPa | |
300% Strain | 3.00 | MPa | |
Tensile Strength (Break) | 9.00 | MPa | ASTM D412 |
Tensile Elongation (Break) | 800 | % | ASTM D412 |
Tear Strength | 30.0 | kN/m | ASTM D624 |
Compression Set | ASTM D395 | ||
23°C, 22 hr | 19 | % | |
70°C, 22 hr | 46 | % | |
100°C, 22 hr | 69 | % |
Flammability | Nominal Value | Test Method | |
---|---|---|---|
Flame Rating | HB | UL 94 |
Injection | Nominal Value | Unit | |
---|---|---|---|
Suggested Max Regrind | 20 | % | |
Rear Temperature | 145 to 175 | °C | |
Middle Temperature | 155 to 185 | °C | |
Front Temperature | 160 to 190 | °C | |
Nozzle Temperature | 175 to 205 | °C | |
Mold Temperature | 25.0 to 50.0 | °C |
Extrusion | Nominal Value | Unit | |
---|---|---|---|
Cylinder Zone 1 Temp. | 150 to 170 | °C | |
Cylinder Zone 2 Temp. | 155 to 175 | °C | |
Cylinder Zone 3 Temp. | 165 to 185 | °C | |
Cylinder Zone 4 Temp. | 175 to 205 | °C | |
Cylinder Zone 5 Temp. | 180 to 210 | °C | |
Die Temperature | 190 to 210 | °C |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
MAJORIS UG600 - 8229 | AD majoris | Nylon 66 | MAJORIS |
POLYPRO® CB5290 | YUHWA Korea Petrochemical Ind. Co., Ltd. | PP Copolymer | POLYPRO® |
Moplen HP526J | LyondellBasell Industries | PP Homopolymer | Moplen |
Felix Compounds Seprene TPE | Felix Compounds | SEEPS | Felix Compounds |
Hostacom EKC 133N KF | LyondellBasell Industries | PP, Unspecified | Hostacom |