| Category: | PVC, Unspecified , Polyvinyl Chloride |
| Manufacturer: | DORLYL S.N.C. |
| Trademark: | Dorlyl PVC |
| Fillers: | - |
| Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
| Delivery Terms | FOB, CIF, DAP, DAT, DDP |
| PDF: | 5Ndxlp_Dorlyl-PVC-GFD-64G.pdf |
| PRICE: | Order Products email sales@su-jiao.com |
| Message |
|---|
|
GFD 64G is a very high transparency, high impact resistance, blush test resistant compound. It is designed for use in bottle blow molding up to nearly 1 l capacity, according to their characteristics. |
| General Information | |
|---|---|
| Features |
|
| Uses |
|
| Agency Ratings |
|
| Appearance |
|
| Forms |
|
| Processing Method |
|
| Physical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Specific Gravity | 1.33 | g/cm³ | ASTM D792 |
| Apparent Density | 0.77 | g/cm³ | ISO 60 |
| Hardness | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Durometer Hardness (Shore D) | 74 | ISO 868 |
| Mechanical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Tensile Stress (Break) | 39.0 | MPa | ISO 527-2 |
| Tensile Strain (Break) | 200 | % | ISO 527-2 |
| Flexural Modulus (23°C) | 2000 | MPa | ISO 178 |
| Impact | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Notched Izod Impact (23°C) | 18 | kJ/m² | ISO 180 |
| Thermal | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Vicat Softening Temperature | 76.0 | °C | ISO 306/B |
| Additional Information |
|---|
| Stabilization: TInVolatile Matter, ISO 1269: <0.2% |
| Resin Grade | Manufacturer | Category | Trademark |
|---|---|---|---|
| RTP 300 MG 20 HF | RTP Company | PC | RTP |
| TAROMID A 280 Z4 | Taro Plast S.p.A. | Nylon 66 | TAROMID A |
| Cevian®-PC 5100 | PlastxWorld Inc. | PC | Cevian®-PC |
| Fainplast PVC GK 86/R | Fainplast Compounds S.r.l | PVC, Flexible | Fainplast PVC |
| Ecodear® V554X51 | Toray Resin Company | PLA | Ecodear® |