Category: | ABS , Acrylonitrile Butadiene Styrene |
Manufacturer: | MBA Polymers |
Trademark: | MBA ABS |
Fillers: | - |
Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
Delivery Terms | FOB, CIF, DAP, DAT, DDP |
PDF: | 4xg6Av_MBA-ABS-4134-70-35-China-.pdf ![]() |
PRICE: | Order Products email sales@su-jiao.com |
Message |
---|
An easy flowing, post-consumer recycled acrylonitrile-butadiene-styrene copolymer for general use. Available in light grey (reference 70/35). |
General Information | |
---|---|
Recycled Content |
|
Features |
|
Uses |
|
Appearance |
|
Forms |
|
Processing Method |
|
Physical | Nominal Value | Unit | Test Method |
---|---|---|---|
Density | 1.06 | g/cm³ | ISO 1183 |
Melt Mass-Flow Rate (MFR) (220°C/10.0 kg) | 22 | g/10 min | ISO 1133 |
Mechanical | Nominal Value | Unit | Test Method |
---|---|---|---|
Tensile Stress (Yield, 23°C) | 40.0 | MPa | ISO 527-2/50 |
Impact | Nominal Value | Unit | Test Method |
---|---|---|---|
Notched Izod Impact Strength (23°C) | 10 | kJ/m² | ISO 180/1A |
Injection | Nominal Value | Unit | |
---|---|---|---|
Drying Temperature | 80.0 | °C | |
Drying Time | 2.0 to 4.0 | hr | |
Suggested Max Moisture | 0.050 to 0.10 | % | |
Processing (Melt) Temp | 210 to 240 | °C | |
Mold Temperature | 40.0 to 60.0 | °C |
Extrusion | Nominal Value | Unit | |
---|---|---|---|
Drying Temperature | 80.0 | °C | |
Drying Time | 2.0 to 4.0 | hr | |
Suggested Max Moisture | 0.050 to 0.10 | % | |
Melt Temperature | 200 to 220 | °C |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
Matrixx WP63E40 | The Matrixx Group, Inc. | Nylon 6 | Matrixx |
Sanren M2500CD (On-spec.) | SINOPEC Shanghai Petrochemical Co. Ltd. | PP Homopolymer | Sanren |
ACLAR® 33C (2 mil) | Honeywell | PCTFE | ACLAR® |
Edgetek™ XT XT-161950602 | PolyOne Corporation | PC+PBT | Edgetek™ XT |
Karina CLEAR PVC COMPOUND 80/208-IS | Karina Ind. e Com. de Plásticos Ltda | PVC, Unspecified | Karina |