| Category: | Nylon 6 , Polyamide 6 |
| Manufacturer: | AD majoris |
| Trademark: | VENYL |
| Fillers: | - |
| Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
| Delivery Terms | FOB, CIF, DAP, DAT, DDP |
| PDF: | 4qZeKA_VENYL-SEG138---7963.pdf |
| PRICE: | Order Products email sales@su-jiao.com |
| Message |
|---|
|
VENYL SEG138 - 7963 is a polyamide 6 impact modified reinforced with 15 % glass fibre intended for injection moulding. APPLICATIONS VENYL SEG138 - 7963 has been developed especially for very demanding applications in automotive industry requiring excellent combination between thermal and mechanical properties. VENYL SEG138 - 7963 is also available in other colours. |
| General Information | |
|---|---|
| Filler / Reinforcement |
|
| Additive |
|
| Features |
|
| Uses |
|
| Appearance |
|
| Forms |
|
| Processing Method |
|
| Physical | Dry | Conditioned | Unit | Test Method |
|---|---|---|---|---|
| Density | 1.19 | -- | g/cm³ | ISO 1183 |
| Molding Shrinkage | 0.50 to 0.90 | -- | % |
| Mechanical | Dry | Conditioned | Unit | Test Method |
|---|---|---|---|---|
| Tensile Modulus | 4750 | 2900 | MPa | ISO 527-2 |
| Tensile Stress (Break) | 95.0 | 65.0 | MPa | ISO 527-2 |
| Tensile Strain (Break) | 4.9 | 8.4 | % | ISO 527-2 |
| Flexural Modulus | 4250 | 2500 | MPa | ISO 178 |
| Flexural Stress | 132 | 85.0 | MPa | ISO 178 |
| Impact | Dry | Conditioned | Unit | Test Method |
|---|---|---|---|---|
| Charpy Notched Impact Strength | 20 | 25 | kJ/m² | ISO 179 |
| Charpy Unnotched Impact Strength | 65 | 95 | kJ/m² | ISO 179 |
| Thermal | Dry | Conditioned | Unit | Test Method |
|---|---|---|---|---|
| Melting Temperature (DSC) | 220 | -- | °C | ISO 3146 |
| Flammability | Dry | Conditioned | Unit | Test Method |
|---|---|---|---|---|
| Flame Rating (1.60 mm) | HB | -- | UL 94 | |
| Glow Wire Flammability Index (2.00 mm) | 650 | -- | °C | IEC 60695-2-12 |
| Injection | Dry | Unit | |
|---|---|---|---|
| Drying Temperature | 90.0 | °C | |
| Drying Time | 4.0 | hr | |
| Rear Temperature | 245 to 265 | °C | |
| Middle Temperature | 250 to 270 | °C | |
| Front Temperature | 255 to 275 | °C | |
| Nozzle Temperature | 255 to 275 | °C | |
| Mold Temperature | 65.0 to 100 | °C | |
| Injection Pressure | 85.0 to 110 | MPa | |
| Injection Rate | Fast | ||
| Holding Pressure | 50.0 to 70.0 | MPa | |
| Screw L/D Ratio | 15.0:1.0 to 20.0:1.0 |
| Resin Grade | Manufacturer | Category | Trademark |
|---|---|---|---|
| RTP 200 D FR | RTP Company | Nylon 612 | RTP |
| Andur AL 90 AP/Curene® 89LC | Anderson Development Company | PUR-Eth,aliphat | Andur |
| APEX® 80-C118Q | Teknor Apex Company | PVC, Flexible | APEX® |
| ESPREE™ ABS7017 | SABIC Innovative Plastics | ABS | ESPREE™ |
| Hostaform® CP15X | Celanese Corporation | Acetal (POM) Copolymer | Hostaform® |