Category: | Nylon 66 , Polyamide 66 |
Manufacturer: | Wellman Engineering Resins |
Trademark: | Wellamid® |
Fillers: | - |
Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
Delivery Terms | FOB, CIF, DAP, DAT, DDP |
PDF: | 4i4LV5_Wellamid-FR22F-NBK3.pdf ![]() |
PRICE: | Order Products email sales@su-jiao.com |
Message |
---|
Wellamid® FR22F-NBK3 is a Polyamide 66 (Nylon 66) material. It is available in Asia Pacific, Europe, Latin America, or North America. Primary attribute of Wellamid® FR22F-NBK3: Flame Retardant. |
General Information | |
---|---|
Features |
|
Forms |
|
Physical | Nominal Value | Unit | Test Method |
---|---|---|---|
Density | 1.32 | g/cm³ | ISO 1183 |
Molding Shrinkage | ISO 294-4 | ||
Across Flow : 23°C | 1.4 to 1.8 | % | |
Flow : 23°C | 1.5 to 1.9 | % |
Mechanical | Nominal Value | Unit | Test Method |
---|---|---|---|
Tensile Stress (Yield, 23°C) | 55.0 | MPa | ISO 527-2 |
Tensile Strain (Yield, 23°C) | 8.0 | % | ISO 527-2 |
Flexural Modulus (23°C) | 3300 | MPa | ISO 178 |
Flexural Stress (23°C) | 90.0 | MPa | ISO 178 |
Impact | Nominal Value | Unit | Test Method |
---|---|---|---|
Notched Izod Impact Strength (23°C) | 3.0 | kJ/m² | ISO 180 |
Thermal | Nominal Value | Unit | Test Method |
---|---|---|---|
Heat Deflection Temperature (1.8 MPa, Unannealed) | 80.0 | °C | ISO 75-2/A |
Melting Temperature (DSC) | 260 | °C | ISO 3146 |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
RTP 383 TFE 5 SE | RTP Company | PC | RTP |
Mylar® S (48 guage) | DuPont Teijin Films U.S. | PET | Mylar® |
Elastron® G G101.A45.N | Elastron USA, Inc. | SEBS | Elastron® G |
Plaslube® J-1/30/TF/15 NAT | Techmer Engineered Solutions | Nylon 66 | Plaslube® |
Tritan™ LX100 | Eastman Chemical Company | Copolyester | Tritan™ |