| Category: | PUR-Ester/TDI , Polyurethane (Polyester, TDI) |
| Manufacturer: | Anderson Development Company |
| Trademark: | Andur |
| Fillers: | - |
| Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
| Delivery Terms | FOB, CIF, DAP, DAT, DDP |
| PDF: | 4fzhlA_Andur-5-DPLM-Curene-442.pdf |
| PRICE: | Order Products email sales@su-jiao.com |
| Message |
|---|
| Andur 5-DPLM is a polyester based, toluene diisocyanate terminated prepolymer. An elastomer with a hardness of 50 Shore D is obtained when this prepolymer is cured with Curene 442 [4,4'-methylene-bis (orthochloroaniline)]. Elastomers of lower hardness can be obtained by curing Andur 5-DPLM with poyols and their combination with Curene 442 and other diamines, or through the use of plasticizers. |
| General Information | |
|---|---|
| Forms |
|
| Physical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Density | 1.23 | g/cm³ | ASTM D1505 |
| Hardness | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Durometer Hardness (Shore D) | 50 | ASTM D2240 |
| Mechanical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Compressive Strength | ASTM D695 | ||
| 5% strain | 0.972 | MPa | ASTM D695 |
| 10% strain | 3.37 | MPa | ASTM D695 |
| 15% strain | 5.58 | MPa | ASTM D695 |
| 25% strain | 8.56 | MPa | ASTM D695 |
| Elastomers | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Tensile Stress | ASTM D412 | ||
| 100% strain | 10.9 | MPa | ASTM D412 |
| 300% strain | 22.7 | MPa | ASTM D412 |
| Tensile Strength (Yield) | 59.1 | MPa | ASTM D412 |
| Tensile Elongation (Break) | 520 | % | ASTM D412 |
| Compression Set | 29 | % | ASTM D395B |
| Bayshore Resilience | 28 | % | ASTM D2632 |
| Thermoset | Nominal Value | Unit | |
|---|---|---|---|
| Pot Life | 3.5 - 5.0 | min | |
| Demold Time | 30 | min | |
| Post Cure Time (96°C) | 16 | hr |
| Additional Information |
|---|
| Durometer Hardness, ASTM D2240, Shore D: 48 to 53Die C Tear, ASTM D1004: 555 pliAverage Split Tear, ASTM D1938: 310 pliStoichiometry Curative Level: 95%Mix Temperature: Andur 5 DPLM: 180-210°F Curene 442: 235-250°F |
| Injection | Nominal Value | Unit | |
|---|---|---|---|
| Mold Temperature | 104 - 113 | °C |
| Resin Grade | Manufacturer | Category | Trademark |
|---|---|---|---|
| Shin-Etsu Elastomer KE-2004-5A/B | Shin-Etsu Silicones of America | Silicone Rubber, HTV | Shin-Etsu Elastomer |
| Spartech Polycom SC5-2220 | Spartech Polycom | PP Copolymer | Spartech |
| ACCUTECH™ TPU030G20V | ACLO Compounders Inc. | TPU, Unspecified | ACCUTECH™ |
| Comtrex Flexible PVC® 71XCF | Mitsubishi Chemical Performance Polymers, Inc. | PVC, Flexible | Comtrex Flexible PVC® |
| Plaslube® PC CF10 TL15 FR BK | Techmer Engineered Solutions | PC | Plaslube® |