| Category: | TPU-Polyether , Thermoplastic Polyurethane Elastomer (Polyether) |
| Manufacturer: | Great Eastern Resins Industrial Co., Ltd. (GRECO) |
| Trademark: | ISOTHANE® |
| Fillers: | - |
| Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
| Delivery Terms | FOB, CIF, DAP, DAT, DDP |
| PDF: | 4eR6u0_ISOTHANE1685AE2.pdf |
| PRICE: | Order Products email sales@su-jiao.com |
| Message |
|---|
| ISOTHANE 1685A-E2 products are polyether based thermoplastic polyurethanes with good balanced qualities. They exhibit high moisture vapor transmission. The product can be extruded and blown. |
| General Information | |
|---|---|
| Features |
|
| Processing Method |
|
| Hardness | Nominal Value | Test Method | |
|---|---|---|---|
| Durometer Hardness (Shore A) | 85 | ASTM D2240 |
| Mechanical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Ross Flex - 150,000 times (-6°C) | No Break | ASTM D1052 |
| Films | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Water Vapor Transmission | |||
| -- | 70000 | g/m²/24 hr | JIS L1099 |
| -- 1 | 11000 | g/m²/24 hr | ASTM E96 |
| Elastomers | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Tensile Stress (300% Strain) | 10.0 | MPa | ASTM D412 |
| Tensile Strength | 23.0 | MPa | ASTM D412 |
| Tensile Elongation (Break) | 850 | % | ASTM D412 |
| Tear Strength 2 | 110 | kN/m | ASTM D624 |
| Extrusion | Nominal Value | Unit | |
|---|---|---|---|
| Drying Temperature | 100 | °C | |
| Drying Time | 3.0 - 4.0 | hr |
| Note Message | |
|---|---|
| 1 . | Procedure BW |
| 2 . | C mould |
| Resin Grade | Manufacturer | Category | Trademark |
|---|---|---|---|
| TEKASTER™ F10G30 | Mando Advanced Materials Co., Ltd. | PBT | TEKASTER™ |
| Softflex® 0470 | Network Polymers, Inc. | TPE | Softflex® |
| Sylvin 2900-68 Clear Green 3181 | Sylvin Technologies Incorporated | PVC, Unspecified | Sylvin |
| Norfor® 130 GF/20 NATURALE 0507 | SO.F.TER. SPA | PPE | Norfor® |
| EPO-TEK® H70E-2LC | Epoxy Technology Inc. | Epoxy | EPO-TEK® |