| Category: | Nylon 6 , Polyamide 6 |
| Manufacturer: | Radici Plastics |
| Trademark: | Radilon® |
| Fillers: | - |
| Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
| Delivery Terms | FOB, CIF, DAP, DAT, DDP |
| PDF: | 4Uqfxc_Radilon-S-RV500.pdf |
| PRICE: | Order Products email sales@su-jiao.com |
| Message |
|---|
| PA6 50% Glass Fiber injection moulding grade. Very high stiffness and dimensional stability. Natural colour |
| General Information | |
|---|---|
| Filler / Reinforcement |
|
| Features |
|
| Appearance |
|
| Forms |
|
| Processing Method |
|
| Physical | Dry | Conditioned | Unit | Test Method |
|---|---|---|---|---|
| Density | 1.54 | -- | g/cm³ | ISO 1183 |
| Water Absorption | ISO 62 | |||
| Saturated, 23°C | 4.8 | -- | % | ISO 62 |
| Equilibrium, 23°C, 50% RH | 1.4 | -- | % | ISO 62 |
| Viscosity Number | 140 | -- | cm³/g | ISO 307 |
| Mechanical | Dry | Conditioned | Unit | Test Method |
|---|---|---|---|---|
| Tensile Modulus | 16400 | 11500 | MPa | ISO 527-2 |
| Tensile Stress (Break) | 220 | 155 | MPa | ISO 527-2 |
| Tensile Strain (Break) | 2.9 | 3.1 | % | ISO 527-2 |
| Impact | Dry | Conditioned | Unit | Test Method |
|---|---|---|---|---|
| Charpy Notched Impact Strength | ISO 179/eA | |||
| -30°C | 17 | -- | kJ/m² | ISO 179/eA |
| 23°C | 18 | 30 | kJ/m² | ISO 179/eA |
| Charpy Unnotched Impact Strength | ISO 179/eU | |||
| -30°C | 100 | -- | kJ/m² | ISO 179/eU |
| 23°C | 110 | 110 | kJ/m² | ISO 179/eU |
| Thermal | Dry | Conditioned | Unit | Test Method |
|---|---|---|---|---|
| Heat Deflection Temperature | ||||
| 0.45 MPa, not annealed | 215 | -- | °C | ISO 75-2/Bf |
| 1.8 MPa, not annealed | 210 | -- | °C | ISO 75-2/Af |
| Vicat Softening Temperature | 215 | -- | °C | ISO 306/B50 |
| Melting Temperature (DSC) | 220 | -- | °C | ISO 3146 |
| Electrical | Dry | Conditioned | Unit | Test Method |
|---|---|---|---|---|
| Surface Resistivity | 1.0E+12 | -- | ohms | IEC 60093 |
| Volume Resistivity | 1.0E+15 | 1.0E+13 | ohms·cm | IEC 60093 |
| Comparative Tracking Index | -- | 550 | V | IEC 60112 |
| Flammability | Dry | Conditioned | Unit | Test Method |
|---|---|---|---|---|
| Flame Rating | UL 94 | |||
| 0.800 mm | HB | -- | UL 94 | |
| 1.60 mm | HB | -- | UL 94 |
| Additional Information |
|---|
| 干燥 The value listed as Melting Temperature, ISO 3146, was tested in accordance with ISO 11357-1-3 at a heating rate of 10°C/min. |
| Resin Grade | Manufacturer | Category | Trademark |
|---|---|---|---|
| UBESTA 3024LU | UBE Industries, Ltd. | Nylon 12 | UBESTA |
| Ferro PP TPP20AJ22UL-NA | Ferro Corporation | PP Homopolymer | Ferro PP |
| Elastollan® 785 A HPM | BASF Polyurethanes GmbH | TPU-Polyester | Elastollan® |
| InnoTuf® TP-4015 | Innovative Polymers, Inc. | TSU | InnoTuf® |
| Sylvin 5132-90UV Clear 8371 | Sylvin Technologies Incorporated | PVC, Unspecified | Sylvin |