| Category: | Nylon 66/6 , Polyamide 66/6 Copolymer |
| Manufacturer: | Solvay Engineering Plastics |
| Trademark: | TECHNYL® |
| Fillers: | - |
| Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
| Delivery Terms | FOB, CIF, DAP, DAT, DDP |
| PDF: | 4MZTi2_TECHNYLB738MX15GREY3279.pdf |
| PRICE: | Order Products email sales@su-jiao.com |
| Message |
|---|
| TECHNYL B 738 MX15 Grey 3279 is a copolyamide 6.6, reinforced with 15% of mineral filler, for injection moulding. This grade offers good mechanical Properties, good superficial aspect and dimensional stability. |
| General Information | |
|---|---|
| Filler / Reinforcement |
|
| Additive |
|
| Features |
|
| Uses |
|
| Appearance |
|
| Forms |
|
| Processing Method |
|
| Resin ID (ISO 1043) |
|
| Physical | Dry | Conditioned | Unit | Test Method |
|---|---|---|---|---|
| Density | 1.22 | -- | g/cm³ | ISO 1183/A |
| Water Absorption (23°C, 24 hr) | 1.2 | -- | % | ISO 62 |
| Mechanical | Dry | Conditioned | Unit | Test Method |
|---|---|---|---|---|
| Tensile Modulus (23°C) | 4300 | -- | MPa | ISO 527-2/1A |
| Tensile Stress (Break, 23°C) | 59.0 | -- | MPa | ISO 527-2/1A |
| Tensile Strain (Break, 23°C) | 3.0 | -- | % | ISO 527-2 |
| Flexural Modulus (23°C) | 3700 | -- | MPa | ISO 178 |
| Flexural Stress (23°C) | 100 | -- | MPa | ISO 178 |
| Impact | Dry | Conditioned | Unit | Test Method |
|---|---|---|---|---|
| Charpy Unnotched Impact Strength (23°C) | 60 | -- | kJ/m² | ISO 179/1eU |
| Thermal | Dry | Conditioned | Unit | Test Method |
|---|---|---|---|---|
| Melting Temperature | 242 | -- | °C | ISO 11357-3 |
| Injection | Dry | Unit | |
|---|---|---|---|
| Drying Temperature | 80 | °C | |
| Suggested Max Moisture | 0.20 | % | |
| Rear Temperature | 255 - 265 | °C | |
| Middle Temperature | 260 - 270 | °C | |
| Front Temperature | 270 - 280 | °C | |
| Mold Temperature | 70 - 100 | °C |
| Injection instructions |
|---|
| The material is supplied in airtight bags, ready for use. In case that the virgin material has absorbed moisture, it must be dried with a dehumidified air drying equipment, dew point mini -20°C. Recommended time 2-4hInjection Advice: For reinforced polyamide, Solvay recommends the use of steel with a high content of Carbon and purified for polishing to avoid or limit the abrasion. For example: X38CrMoV5-1 (EN Norm) - 1.2367 /1.2343 (DIN Norm) or X160CrMoV12 (EN Norm) - 1.2601 /1.2379 (DIN Norm). For Mould Temperature, in the case of parts where the surface roughness is required we can recommend a temperature of 90°C to 120°C with an optimum at 105°C. |
| Resin Grade | Manufacturer | Category | Trademark |
|---|---|---|---|
| RTP ESD C 1480 N | RTP Company | PESU | RTP |
| Shuang-Bang WM-8155N | Shuang-Bang Industrial Corp. | Film, TPU | Shuang-Bang |
| STERLENE™ CMV208 | R&P (Pte.) Ltd. | TPO (POE) | STERLENE™ |
| ALTECH® PA6 A 4230/140 MR20 GF10 FR | ALBIS PLASTIC GmbH | Nylon 6 | ALTECH® PA6 |
| LNP™ THERMOCOMP™ DB008ERP compound | SABIC Innovative Plastics | PC | LNP™ THERMOCOMP™ |