| Category: | Nylon 6 , Polyamide 6 |
| Manufacturer: | A. Schulman Europe |
| Trademark: | SCHULAMID® |
| Fillers: | - |
| Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
| Delivery Terms | FOB, CIF, DAP, DAT, DDP |
| PDF: | 4Lu9cQ_SCHULAMID-6-GF-30-HI-WIT.pdf |
| PRICE: | Order Products email sales@su-jiao.com |
| Message |
|---|
| 30% glass fiber reinforced high impact Polyamide 6, optimized for WIT-processes |
| General Information | |
|---|---|
| Filler / Reinforcement |
|
| Features |
|
| Processing Method |
|
| Physical | Dry | Conditioned | Unit | Test Method |
|---|---|---|---|---|
| Density | 1.32 | -- | g/cm³ | ISO 1183/A |
| Mechanical | Dry | Conditioned | Unit | Test Method |
|---|---|---|---|---|
| Tensile Modulus | 7400 | 5000 | MPa | ISO 527-2/1A/1 |
| Tensile Stress (Break) | 115 | 85.0 | MPa | ISO 527-2/1A/5 |
| Tensile Strain (Break) | 4.0 | 10 | % | ISO 527-2/1A/5 |
| Impact | Dry | Conditioned | Unit | Test Method |
|---|---|---|---|---|
| Charpy Notched Impact Strength | ISO 179/1eA | |||
| -30°C | 10 | -- | kJ/m² | |
| 23°C | 14 | 20 | kJ/m² | |
| Charpy Unnotched Impact Strength | ISO 179/1eU | |||
| -30°C | 70 | -- | kJ/m² | |
| 23°C | 75 | 80 | kJ/m² |
| Thermal | Dry | Conditioned | Unit | Test Method |
|---|---|---|---|---|
| Heat Deflection Temperature (1.8 MPa, Unannealed) | 185 | -- | °C | ISO 75-2/Af |
| Vicat Softening Temperature | 200 | -- | °C | ISO 306/B50 |
| Electrical | Dry | Conditioned | Unit | Test Method |
|---|---|---|---|---|
| Surface Resistivity | > 1.0E+15 | -- | ohms | IEC 60093 |
| Volume Resistivity | > 1.0E+13 | > 1.0E+10 | ohms·cm | IEC 60093 |
| Resin Grade | Manufacturer | Category | Trademark |
|---|---|---|---|
| TRIBIT® 1500G20K | Samyang Corporation | PBT | TRIBIT® |
| ACRYLITE® MD™ L40 | Evonik Cyro LLC | Acrylic (PMMA) | ACRYLITE® MD™ |
| Braskem PP TI4020N | Braskem America Inc. | PP Impact Copolymer | Braskem PP |
| Ipiranga GF 4960 | Braskem | HDPE | Ipiranga |
| Jackdaw PLA HS10VN6587 | Jackdaw Polymers | PLA | Jackdaw PLA |