Glass Filled Impact Modified Nylon 12 Features:
Applications:
|
General Information | |
---|---|
Filler / Reinforcement |
|
Features |
|
Uses |
|
Processing Method |
|
Physical | Nominal Value | Unit | Test Method |
---|---|---|---|
Specific Gravity | 1.14 | g/cm³ | ASTM D792 |
Molding Shrinkage - Flow | 0.25 to 0.45 | % | ASTM D955 |
Water Absorption (24 hr) | 0.60 | % | ASTM D570 |
Mechanical | Nominal Value | Unit | Test Method |
---|---|---|---|
Tensile Strength (Yield) | 58.6 | MPa | ASTM D638 |
Tensile Elongation (Break) | 8.5 | % | ASTM D638 |
Flexural Modulus | 2210 | MPa | ASTM D790 |
Flexural Strength | 72.4 | MPa | ASTM D790 |
Impact | Nominal Value | Unit | Test Method |
---|---|---|---|
Notched Izod Impact (23°C, 3.18 mm) | 140 | J/m | ASTM D256 |
Unnotched Izod Impact (23°C, 3.18 mm) | 440 | J/m | ASTM D256 |
Injection | Nominal Value | Unit | |
---|---|---|---|
Drying Temperature | 76.7 | °C | |
Drying Time | 4.0 to 8.0 | hr | |
Rear Temperature | 238 to 260 | °C | |
Middle Temperature | 243 to 266 | °C | |
Front Temperature | 249 to 271 | °C | |
Nozzle Temperature | 243 to 266 | °C | |
Processing (Melt) Temp | 243 to 266 | °C | |
Mold Temperature | 54.4 to 82.2 | °C | |
Injection Rate | Moderate-Fast | ||
Screw Speed | 20 to 100 | rpm | |
Clamp Tonnage | 4.1 to 6.9 | kN/cm² |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
Evoprene™ G 996 | AlphaGary | SEBS | Evoprene™ G |
Eltex® B4020N1332 | INEOS Olefins & Polymers Europe | HDPE Copolymer | Eltex® |
Jackdaw PC DS20WT6701 | Jackdaw Polymers | PC+PBT | Jackdaw PC |
Jam PE 60511 | Jam Petrochemical Company | LLDPE | Jam PE |
Petlon Prime B1-G15-00-BK | Petlon Polymers Ltd | Nylon 6 | Petlon Prime |