| Category: | Polyester, TP , Thermoplastic Polyester |
| Manufacturer: | Crosspolimeri S.p.A. |
| Trademark: | TRELGUM |
| Fillers: | - |
| Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
| Delivery Terms | FOB, CIF, DAP, DAT, DDP |
| PDF: | 3yKQmM_TRELGUM-ME-9-DP-2Z.pdf |
| PRICE: | Order Products email sales@su-jiao.com |
| Message |
|---|
|
TRELGUM ME/9 DP 2Z is a modified polyester technopolymer presenting in itself the relevant features of both rubbers and plasticized materials. TRELGUM ME/9 DP 2Z is a tough compound showing good resistance properties to deformation, compression and to flex-fatigue. It also has good abrasion resistance and resistance to many chemicals and oils. |
| General Information | |
|---|---|
| Features |
|
| Uses |
|
| Forms |
|
| Processing Method |
|
| Physical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Specific Gravity | 1.18 | g/cm³ | ASTM D792 |
| Hardness | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Durometer Hardness (Shore A) | 71 | ASTM D2240 |
| Mechanical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Tensile Strength | 16.5 | MPa | ASTM D638 |
| Tensile Elongation (Break) | 390 | % | ASTM D638 |
| Elastomers | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Compression Set (70°C, 22 hr) | 60 | % | NES 715 |
| Aging | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Change in Tensile Strength in Air (120°C, 168 hr) | 25 | % | IEC 60811 |
| Change in Tensile Strain at Break in Air (120°C, 168 hr) | -20 | % | IEC 60811 |
| Change in Tensile Stress (120°C, 168 hr, in ASTM #2 Oil) | 30 | % | IEC 60811 |
| Change in Tensile Strain at Break (120°C, 168 hr, in ASTM #2 Oil) | 35 | % | IEC 60811 |
| Thermal | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Cold Flexibility | -50 | °C | ASTM D1043 |
| Electrical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Volume Resistivity | 1.5E+12 | ohms·cm | BS 6622 |
| Extrusion | Nominal Value | Unit | |
|---|---|---|---|
| Cylinder Zone 1 Temp. | 160 | °C | |
| Cylinder Zone 2 Temp. | 165 | °C | |
| Cylinder Zone 3 Temp. | 170 | °C | |
| Cylinder Zone 4 Temp. | 170 | °C | |
| Cylinder Zone 5 Temp. | 170 to 175 | °C | |
| Die Temperature | 175 to 185 | °C |
| Resin Grade | Manufacturer | Category | Trademark |
|---|---|---|---|
| Starflam BFR552Y3 | Eurostar Engineering Plastics | Nylon 6 | Starflam |
| Sylvin 6209-80 Natural | Sylvin Technologies Incorporated | PVC, Unspecified | Sylvin |
| Fainplast PVC RK 126/X | Fainplast Compounds S.r.l | PVC, Rigid | Fainplast PVC |
| Hostacom M4 N01 L303612 | LyondellBasell Industries | PP Homopolymer | Hostacom |
| LUVOCOM® 1-1141 | Lehmann & Voss & Co. | Nylon 66 | LUVOCOM® |