Category: | PBT , Polybutylene Terephthalate |
Manufacturer: | RTP Company |
Trademark: | RTP |
Fillers: | - |
Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
Delivery Terms | FOB, CIF, DAP, DAT, DDP |
PDF: | 3r1VaR_RTP-1000-HI-UV.pdf ![]() |
PRICE: | Order Products email sales@su-jiao.com |
Message |
---|
Warning: The status of this material is 'Commercial: Limited Issue' The data for this material has not been recently verified. Please contact RTP Company for current information prior to specifying this grade. -Preliminary Product Data per RTP Co.- |
General Information | |
---|---|
Additive |
|
Features |
|
RoHS Compliance |
|
Appearance |
|
Forms |
|
Processing Method |
|
Physical | Nominal Value | Unit | Test Method |
---|---|---|---|
Specific Gravity | 1.22 | g/cm³ | ASTM D792 |
Molding Shrinkage - Flow (3.18 mm) | 1.5 | % | ASTM D955 |
Water Absorption (23°C, 24 hr) | 0.080 | % | ASTM D570 |
Hardness | Nominal Value | Unit | Test Method |
---|---|---|---|
Rockwell Hardness (R-Scale) | 115 | ASTM D785 |
Mechanical | Nominal Value | Unit | Test Method |
---|---|---|---|
Tensile Modulus | 1720 | MPa | ASTM D638 |
Tensile Strength | 34.5 | MPa | ASTM D638 |
Tensile Elongation (Break) | 10 | % | ASTM D638 |
Flexural Modulus | 1520 | MPa | ASTM D790 |
Flexural Strength | 48.3 | MPa | ASTM D790 |
Impact | Nominal Value | Unit | Test Method |
---|---|---|---|
Notched Izod Impact (3.18 mm) | 960 | J/m | ASTM D256 |
Unnotched Izod Impact (3.18 mm) | No Break | ASTM D4812 |
Thermal | Nominal Value | Unit | Test Method |
---|---|---|---|
Deflection Temperature Under Load | ASTM D648 | ||
0.45 MPa, not annealed | 121 | °C | ASTM D648 |
1.8 MPa, not annealed | 48.9 | °C | ASTM D648 |
Electrical | Nominal Value | Unit | Test Method |
---|---|---|---|
Volume Resistivity | 1.0E+16 | ohms·cm | ASTM D257 |
Flammability | Nominal Value | Unit | Test Method |
---|---|---|---|
Flame Rating (1.59 mm) | HB | UL 94 |
Additional Information |
---|
Mold Shrinkage, Linear-Flow, ASTM D-955, 0.25in.: 20mil/in. |
Injection | Nominal Value | Unit | |
---|---|---|---|
Drying Temperature | 121 | °C | |
Drying Time | 4.0 | hr | |
Suggested Max Moisture | 0.030 | % | |
Suggested Max Regrind | 20 | % | |
Rear Temperature | 232 - 271 | °C | |
Middle Temperature | 232 - 271 | °C | |
Front Temperature | 232 - 271 | °C | |
Mold Temperature | 37.8 - 65.6 | °C | |
Injection Pressure | 68.9 - 103 | MPa |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
PROTEQ™ C16UST22L | Marplex Australia Pty. Ltd. | PP Copolymer | PROTEQ™ |
Radilon® A RV300FC 100 NAT 4792 | Radici Plastics | Nylon 66 | Radilon® |
Moplen EP549N | HMC Polymers | PP Impact Copolymer | Moplen |
Bergamid™ B650 G/Mi20 UF | PolyOne Corporation | Nylon 6 | Bergamid™ |
APEX® 1004 | Teknor Apex Company | PVC, Flexible | APEX® |