Category: | PP Homopolymer , Polypropylene Homopolymer |
Manufacturer: | Polykemi AB |
Trademark: | POLYfill |
Fillers: | - |
Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
Delivery Terms | FOB, CIF, DAP, DAT, DDP |
PDF: | 3pfft3_POLYfill-PPH-T15040CR.pdf ![]() |
PRICE: | Order Products email sales@su-jiao.com |
Message |
---|
Mineral reinforced |
General Information | |
---|---|
Filler / Reinforcement |
|
Physical | Nominal Value | Unit | Test Method |
---|---|---|---|
Density | 1.23 | g/cm³ | ISO 1183 |
Melt Mass-Flow Rate (MFR) (230°C/2.16 kg) | 15 | g/10 min | ISO 1133 |
Molding Shrinkage | ISO 294-4 | ||
Across Flow | 0.80 to 1.0 | % | |
Flow | 0.80 to 1.0 | % |
Mechanical | Nominal Value | Unit | Test Method |
---|---|---|---|
Tensile Stress | 29.0 | MPa | ISO 527-2 |
Tensile Strain (Yield) | 4.0 | % | ISO 527-2 |
Flexural Modulus (23°C) | 3900 | MPa | ISO 178 |
Flexural Stress | 58.0 | MPa | ISO 178 |
Impact | Nominal Value | Unit | Test Method |
---|---|---|---|
Charpy Notched Impact Strength | ISO 179 | ||
-20°C | 1.5 | kJ/m² | |
23°C | 2.0 | kJ/m² |
Thermal | Nominal Value | Unit | Test Method |
---|---|---|---|
Heat Deflection Temperature 1 | |||
0.45 MPa, Unannealed | 125 | °C | ISO 75-2/B |
1.8 MPa, Unannealed | 75.0 | °C | ISO 75-2/A |
Vicat Softening Temperature | |||
-- | 148 | °C | ISO 306/A50 |
-- | 88.0 | °C | ISO 306/B50 |
Flammability | Nominal Value | Unit | Test Method |
---|---|---|---|
Flame Rating (1.60 mm) | HB | UL 94 | |
Glow Wire Ignition Temperature (2.00 mm) | 750 | °C | IEC 60695-2-13 |
Note Message | |
---|---|
1 . | 120°C/hr |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
QR Resin QR-9046-GF15 | QTR, Inc. | Nylon 46 | QR Resin |
Tectron H2456 | TECTRON Systems Pte Ltd | TPV | Tectron |
MTM® 29SFR | Cytec Industries Inc. | Epoxy | MTM® |
Di-Pak™ E-4889 | Hapco Inc. | TP, Unspecified | Di-Pak™ |
Elastron® D D101.A53.N | Elastron USA, Inc. | SBS | Elastron® D |