Category: | TPV , Thermoplastic Vulcanizate |
Manufacturer: | Teknor Apex Company |
Trademark: | Sarlink® TPV |
Fillers: | - |
Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
Delivery Terms | FOB, CIF, DAP, DAT, DDP |
PDF: | 3itkMp_Sarlink-TPV-11044DB.pdf ![]() |
PRICE: | Order Products email sales@su-jiao.com |
Message |
---|
The Sarlink 11000 Series of slip coating materials offer extremely low coefficient of friction against glass, and can be co-extruded with TPE-S, TPE-V, and EPDM. |
General Information | |
---|---|
Features |
|
Uses |
|
Appearance |
|
Forms |
|
Processing Method |
|
Physical | Nominal Value | Unit | Test Method |
---|---|---|---|
Density | 0.960 | g/cm³ | ASTM D792 |
Hardness | Nominal Value | Unit | Test Method |
---|---|---|---|
Shore Hardness (Shore D, 5 sec, Injection Molded) | 40 | ASTM D2240 |
Mechanical | Nominal Value | Unit | Test Method |
---|---|---|---|
Flexural Modulus | 173 | MPa | ASTM D790 |
Coefficient of Friction (vs. Glass - Dynamic) | 0.28 | ASTM D1894 |
Elastomers | Nominal Value | Unit | Test Method |
---|---|---|---|
Tensile Strength - Across Flow (Break) | 11.0 | MPa | ASTM D412 |
Tensile Elongation - Across Flow (Break) | 550 | % | ASTM D412 |
Fill Analysis | Nominal Value | Unit | Test Method |
---|---|---|---|
Apparent Viscosity (200°C, 206 sec^-1) | 312 | Pa·s | ASTM D3835 |
Extrusion | Nominal Value | Unit | |
---|---|---|---|
Cylinder Zone 1 Temp. | 177 to 210 | °C | |
Cylinder Zone 2 Temp. | 182 to 216 | °C | |
Cylinder Zone 3 Temp. | 193 to 227 | °C | |
Cylinder Zone 5 Temp. | 193 to 227 | °C | |
Die Temperature | 193 to 227 | °C |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
Vital-Line SME14455 | Teknor Apex Asia Pacific PTE. LTD. | PVC, Flexible | Vital-Line |
Keltan® 4450S | LANXESS Buna GmbH | EPDM | Keltan® |
KMI PP KM-616IB | KMI Group, Inc. | PP Impact Copolymer | KMI PP |