| Category: | Nylon 6 , Polyamide 6 |
| Manufacturer: | Kolon Plastics, Inc. |
| Trademark: | KOPA® |
| Fillers: | - |
| Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
| Delivery Terms | FOB, CIF, DAP, DAT, DDP |
| PDF: | 3fy0nf_KOPAKN133G20HIBK.pdf |
| PRICE: | Order Products email sales@su-jiao.com |
| Message |
|---|
| Middle viscosity, Impact Resistant, G/F 20% reinforced, Black color |
| General Information | |
|---|---|
| Filler / Reinforcement |
|
| Features |
|
| Appearance |
|
| Processing Method |
|
| Physical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Density | 1.26 | g/cm³ | ISO 1183 |
| Mechanical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Tensile Stress (23°C) | 120 | MPa | ISO 527-2 |
| Tensile Strain (Break, 23°C) | 2.0 | % | ISO 527-2 |
| Flexural Modulus (23°C) | 4900 | MPa | ISO 178 |
| Flexural Stress (23°C) | 170 | MPa | ISO 178 |
| Impact | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Charpy Notched Impact Strength (23°C) | 12 | kJ/m² | ISO 179/1eA |
| Thermal | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Heat Deflection Temperature (1.8 MPa, Unannealed) | 182 | °C | ISO 75-2/A |
| Melting Temperature | 220 | °C | ISO 11357-3 |
| Injection | Nominal Value | Unit | |
|---|---|---|---|
| Drying Temperature - Desiccant Dryer | 80 - 100 | °C | |
| Drying Time - Desiccant Dryer | 4.0 - 5.0 | hr | |
| Suggested Max Moisture | < 0.050 | % | |
| Rear Temperature | 230 | °C | |
| Middle Temperature | 245 | °C | |
| Front Temperature | 250 | °C | |
| Nozzle Temperature | 255 | °C | |
| Mold Temperature | 60 - 80 | °C |
| Resin Grade | Manufacturer | Category | Trademark |
|---|---|---|---|
| PRL PC-HH-UV | Polymer Resources Ltd. | PC | PRL |
| Quadrant EPP Nylatron® GSM Blue | Quadrant Engineering Plastic Products | Nylon 6 | Quadrant EPP |
| Versalloy™ HC 9210-55N | PolyOne Corporation | TPE | Versalloy™ |
| POCAN® BF 4225 000000 | LANXESS Corporation | PBT | POCAN® |
| LEXAN™ FXM121R resin | SABIC Innovative Plastics Europe | PC | LEXAN™ |