| Message |
|---|
| POM Copolymer, 30% mineral reinforced |
| General Information | |
|---|---|
| Filler / Reinforcement |
|
| Resin ID (ISO 1043) |
|
| Physical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Density | 1.58 | g/cm³ | ISO 1183 |
| Melt Mass-Flow Rate (MFR) (190°C/2.16 kg) | 22 | g/10 min | ISO 1133 |
| Molding Shrinkage | ISO 294-4 | ||
| Across Flow | 1.5 | % | |
| Flow | 1.2 | % |
| Mechanical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Tensile Modulus | 4700 | MPa | ISO 527-2 |
| Tensile Stress (Break) | 60.0 | MPa | ISO 527-2 |
| Tensile Strain (Break) | 11 | % | ISO 527-2 |
| Impact | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Charpy Notched Impact Strength (23°C) | 5.0 | kJ/m² | ISO 179/1eA |
| Thermal | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Heat Deflection Temperature (1.8 MPa, Unannealed) | 145 | °C | ISO 75-2/A |
| Melting Temperature 1 | 166 | °C | ISO 11357-3 |
| Note Message | |
|---|---|
| 1 . | 10°C/min |
| Resin Grade | Manufacturer | Category | Trademark |
|---|---|---|---|
| RTP 300 L Z | RTP Company | PC | RTP |
| RTP EMI 361 | RTP Company | PC | RTP |
| TAROMID A 280 | Taro Plast S.p.A. | Nylon 66 | TAROMID A |
| Jam PE 12HF6 | Jam Petrochemical Company | LLDPE | Jam PE |
| Sylvin 8230-90LG Black | Sylvin Technologies Incorporated | PVC, Unspecified | Sylvin |