| Category: | Nylon 66/6 , Polyamide 66/6 Copolymer |
| Manufacturer: | Wellman Engineering Resins |
| Trademark: | Wellamid® |
| Fillers: | - |
| Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
| Delivery Terms | FOB, CIF, DAP, DAT, DDP |
| PDF: | 3LEPe9_Wellamid-GF43-66-6-XE-NBK1.pdf |
| PRICE: | Order Products email sales@su-jiao.com |
| Message |
|---|
|
Wellamid® GF43-66/6 XE-NBK1 is a Polyamide 66/6 Copolymer (Nylon 66/6) material filled with 43% glass fiber. It is available in Asia Pacific, Europe, Latin America, or North America. Typical application of Wellamid® GF43-66/6 XE-NBK1: Automotive |
| General Information | |
|---|---|
| Filler / Reinforcement |
|
| Forms |
|
| Physical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Density | 1.50 | g/cm³ | ISO 1183 |
| Molding Shrinkage | ISO 294-4 | ||
| Across Flow : 23°C | 0.70 to 1.1 | % | |
| Flow : 23°C | 0.10 to 0.50 | % |
| Mechanical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Tensile Stress (Yield, 23°C) | 175 | MPa | ISO 527-2 |
| Tensile Strain (Yield, 23°C) | 2.0 | % | ISO 527-2 |
| Flexural Modulus (23°C) | 11900 | MPa | ISO 178 |
| Flexural Stress (23°C) | 260 | MPa | ISO 178 |
| Impact | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Notched Izod Impact Strength (23°C) | 11 | kJ/m² | ISO 180 |
| Thermal | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Heat Deflection Temperature (1.8 MPa, Unannealed) | 225 | °C | ISO 75-2/A |
| Melting Temperature (DSC) | 260 | °C | ISO 3146 |
| Resin Grade | Manufacturer | Category | Trademark |
|---|---|---|---|
| RANPELEN SFC-750M | Lotte Chemical Corporation | PP Terpolymer | RANPELEN |
| Telcar® TL-1425A | Teknor Apex Company | TPE | Telcar® |
| ALCUDIA® LDPE 1970C | REPSOL | LDPE | ALCUDIA® LDPE |
| Hyflon® PFA P7010 | Solvay Specialty Polymers | PFA | Hyflon® PFA |
| LNP™ STAT-KON™ DE006 compound | SABIC Innovative Plastics Europe | PC | LNP™ STAT-KON™ |