| Category: | PVC, Unspecified , Polyvinyl Chloride |
| Manufacturer: | Sylvin Technologies Incorporated |
| Trademark: | Sylvin |
| Fillers: | - |
| Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
| Delivery Terms | FOB, CIF, DAP, DAT, DDP |
| PDF: | 3GGD0r_Sylvin514575ClearRed6192.pdf |
| PRICE: | Order Products email sales@su-jiao.com |
| Message |
|---|
| Sylvin 5145-75 Clear Red 6192 Is A Vinyl Compound Formulated For Speaker Wire Applications. |
| General Information | |
|---|---|
| Uses |
|
| Appearance |
|
| Processing Method |
|
| Physical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Specific Gravity | 1.20 | g/cm³ | ASTM D792 |
| Hardness | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Durometer Hardness | ASTM D2240 | ||
| Shaw A | 75 | ASTM D2240 | |
| Shaw A, 10 seconds | 75 | ASTM D2240 |
| Mechanical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Tensile Strength (Break) | 15.9 | MPa | ASTM D638 |
| Tensile Elongation (Break) | 430 | % | ASTM D638 |
| Elastomers | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Tear Strength | 61.3 | kN/m | ASTM D624 |
| Thermal | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Continuous Use Temperature | 105 | °C | ASTM D794 |
| Melting Temperature | 163 - 174 | °C |
| Flammability | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Oxygen Index | 22 | % | ASTM D2863 |
| Resin Grade | Manufacturer | Category | Trademark |
|---|---|---|---|
| SKYBOND® 700 | Industrial Summit Technology Co. | API | SKYBOND® |
| Toyolac® 250-X10 | Toray Resin Company | ABS | Toyolac® |
| ENFLEX V1030A | ENPLAST Americas, a Ravago Group Company | TPV | ENFLEX |
| Hostaform® EC140XF | Celanese Corporation | Acetal (POM) Copolymer | Hostaform® |
| TECHNYL® C 256 V18 (EX PSB 197) NATURAL | Solvay Engineering Plastics | Nylon 6 | TECHNYL® |